Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ALCOM PBT 700/1.1 CF20 PTFE15 - (PBT+PTFE)-CF20 - MOCOM Compounds GmbH & Co. KG

Material Data Center offers the following functions for ALCOM PBT 700/1.1 CF20 PTFE15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Alcom datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
材料类型聚对苯二甲酸丁二醇酯
填充/添加剂体系20 % 碳纤,15 % PTFE
主要特征导电,较低的表面电阻率,提高的滑动/耐磨性能,热老化稳定性
市场分类机械
应用范围注塑部件
主要应用外壳件,功能部件
机械性能价值单位Test Standard
ISO数据
拉伸模量 16200 MPa ISO 527
断裂应力 140 MPa ISO 527
断裂伸长率 1.6 % ISO 527
无缺口简支梁冲击强度, +23°C 37 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 6 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 217 °C ISO 75-1/-2
维卡软化温度, B 210 °C ISO 306
电性能价值单位Test Standard
ISO数据
表面电阻率 25 Ohm IEC 62631-3-2
其它性能价值单位Test Standard
密度 1470 kg/m³ ISO 1183
典型数据
加工方法
注塑
特殊性能
提高导电性
地区供应
其他信息
注塑成型
烘干条件在干燥空气(除湿)干燥器里 100-120 °C
for 2-4 h
在循环空气干燥器里 100-120 °C
for 4-8 h
取决于湿度含量
注塑成型工艺注塑熔体温度 250-270 °C
注塑模具温度 80-120 °C
储存干燥,避免光照
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.