Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VALOX™ FR Resin ENH8560 - Europe - (PBT+PET)-GF30 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for VALOX™ FR Resin ENH8560 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Valox datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
VALOX ENH8560 is a 30% glass reinforced, non-chlorinated/brominated flame retardant Polybutylene Terephthalate/Polyethylene Terephthalate (PBT/PET) injection moldable grade with excellent chemical resistance. It has a UL94V0@1.5mm and 5VA@2.0mm flame rating. This is a good candidate for a variety of applications needing a sustainable FR PBT/PET solution.

UL Yellow Card Link E45329-100705592
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 25 cm³/10min ISO 1133
温度 265 °C -
载荷 5 kg -
熔融指数, MFI 11 g/10min ISO 1133
温度 250 °C -
负载 5 kg -
ASTM数据
熔融指数, MFI 5 g/10min ASTM D 1238
温度 265 °C -
负载 2.16 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 12000 MPa ISO 527
屈服应力 105 MPa ISO 527
屈服伸长率 1 % ISO 527
断裂应力 105 MPa ISO 527
断裂伸长率 2 % ISO 527
弯曲模量 10000 MPa ISO 178
简支梁缺口冲击强度, +23°C 5 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm 30 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 27 kJ/m² ISO 180/1U
悬臂梁缺口冲击强度, +23°C, 4mm 7 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, -30°C, 4mm 7 kJ/m² ISO 180/1A
洛克硬度 R 118 - ISO 2039-2
球压硬度 166 MPa ISO 2039-1
ASTM数据
拉伸模量 12000 MPa ASTM D 638
屈服应力 103 MPa ASTM D 638
断裂拉伸强度 103 MPa ASTM D 638
屈服伸长率 1 % ASTM D 638
断裂伸长率 2 % ASTM D 638
弯曲模量 10000 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 60 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 60 J/m ASTM D 256
温度 -30 °C -
Izod冲击强度, 1/8 in 450 J/m ASTM D 256
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 180 °C ISO 75-1/-2
热变形温度, 0.45 MPa 215 °C ISO 75-1/-2
维卡软化温度, A 215 °C ISO 306
维卡软化温度, B 203 °C ISO 306
维卡软化温度, 120°C/h 50N 201 °C ISO 306
1.5mm名义厚度时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
厚度为h时的5V燃烧性 5VA class IEC 60695-11-20
测试用试样的厚度 2.0 mm -
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
灼热丝引燃温度 (GWIT) 750 °C IEC 60695-2-13
GWIT - 测试用试样厚度 1 mm -
灼热丝引燃温度 (GWIT) 775 °C IEC 60695-2-13
GWIT - 测试用试样厚度 2 mm -
灼热丝引燃温度 (GWIT) 825 °C IEC 60695-2-13
GWIT - 测试用试样厚度 3 mm -
ASTM数据
DTUL @ 66 psi 210 °C ASTM D 648
DTUL @ 264 psi 196 °C ASTM D 648
维卡温度 196 °C ASTM D 1525
电性能价值单位Test Standard
ISO数据
相对介电常数, 1MHz 3.6 - IEC 62631-2-1
介质损耗因子, 1MHz 120 E-4 IEC 62631-2-1
体积电阻率 1E13 Ohm*m IEC 62631-3-1
表面电阻率 >1E15 Ohm IEC 62631-3-2
介电强度 35 kV/mm IEC 60243-1
相对漏电起痕指数 425 - IEC 60112
ASTM数据
电介质强度, 短时 8 kV/mm ASTM D 149
耗散因素, 1 MHz 0.012 - ASTM D 150
电介质常数, 1 MHz 3.6 - ASTM D 150
体积电阻率 1E15 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
吸水性 0.3 % 类似ISO 62
吸湿性 0.05 % 类似ISO 62
密度 1580 kg/m³ ISO 1183
吸水率, 24小时 0.07 % ASTM D 570
密度 1580 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 110 - 120 °C -
预干燥-时间 4 - 6 h -
加工湿度 ≤0.02 % -
注塑熔体温度 260 - 285 °C -
模具温度 60 - 110 °C -
加料温度 40 - 60 °C -
1区 240 - 260 °C -
2区 255 - 280 °C -
3区 260 - 280 °C -
典型数据
加工方法
注塑
添加剂
阻燃剂
特殊性能
阻燃的
耐化学试剂
通用耐化学性
地区供应
欧洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.