Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin PX9406K - Asia - (PPE+PS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin PX9406K - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
NORYL PX9406K resin may be suitable for consumer electronics applications. Flame retardant used is non-halogenated. UL94 V0 at 1.5 mm, 5VB at 2 mm, and 5VA at 2.5 mm. RTI (impact) = 105 C

UL Yellow Card Link E207780-101401128
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 11 cm³/10min ISO 1133
温度 280 °C -
载荷 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2550 MPa ISO 527
屈服应力 67 MPa ISO 527
屈服伸长率 5 % ISO 527
断裂应力 52 MPa ISO 527
断裂伸长率 50 % ISO 527
弯曲模量 2420 MPa ISO 178
简支梁缺口冲击强度, +23°C 13 kJ/m² ISO 179/1eA
简支梁缺口冲击强度, -30°C 5 kJ/m² ISO 179/1eA
悬臂梁缺口冲击强度, +23°C, 4mm 12 kJ/m² ISO 180/1A
悬臂梁缺口冲击强度, -30°C, 4mm 5 kJ/m² ISO 180/1A
ASTM数据
拉伸模量 2700 MPa ASTM D 638
屈服应力 66 MPa ASTM D 638
断裂拉伸强度 50 MPa ASTM D 638
屈服伸长率 5.7 % ASTM D 638
断裂伸长率 45 % ASTM D 638
弯曲模量 2650 MPa ASTM D 790
悬臂梁缺口冲击强度, 1/8 in 170 J/m ASTM D 256
低温悬臂梁缺口冲击强度, Low-Temperature 100 J/m ASTM D 256
温度 -30 °C -
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 111 °C ISO 75-1/-2
维卡软化温度, 120°C/h 10N 144 °C ISO 306
维卡软化温度, 120°C/h 50N 134 °C ISO 306
1.5mm名义厚度时的燃烧性 V-0 class IEC 60695-11-10
测试用试样的厚度 1.5 mm -
厚度为h时的5V燃烧性 5VB class IEC 60695-11-20
测试用试样的厚度 2.0 mm -
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
灼热丝燃烧指数 (GWFI) 960 °C IEC 60695-2-12
灼热丝引燃温度 (GWIT) 800 °C IEC 60695-2-13
GWIT - 测试用试样厚度 2 mm -
灼热丝引燃温度 (GWIT) 800 °C IEC 60695-2-13
GWIT - 测试用试样厚度 3 mm -
ASTM数据
DTUL @ 66 psi 128 °C ASTM D 648
DTUL @ 264 psi 113 °C ASTM D 648
电性能价值单位Test Standard
ISO数据
相对漏电起痕指数 250 - IEC 60112
ASTM数据
体积电阻率 >1E15 Ohm*cm ASTM D 257
其它性能价值单位Test Standard
密度 1100 kg/m³ ISO 1183
密度 1100 kg/m³ ASTM D 792
加工推荐(注塑)价值单位Test Standard
预干燥-温度 105 - 110 °C -
预干燥-时间 3 - 4 h -
加工湿度 ≤0.02 % -
注塑熔体温度 275 - 305 °C -
模具温度 70 - 100 °C -
1区 245 - 295 °C -
2区 255 - 300 °C -
3区 265 - 305 °C -
螺杆转速 20 - 100 rpm -
背压 0.3 - 0.7 MPa -
典型数据
加工方法
注塑
添加剂
阻燃剂
特殊性能
阻燃的
地区供应
亚太
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.