Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Borlink" in Material Data Center leads to the following information:

Tradename: Borlink
Family: PE-X
Producer: Borealis AS
32 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Borlink™ LC8205R PE
Borlink™ LE0315 PE
Borlink™ LE0500 PE
Borlink™ LE0511 PE
Borlink™ LE0516 PE
Borlink™ LE0520 PE
Borlink™ LE0550DC PE
Borlink™ LE0592 PE
Borlink™ LE0592S PE
Borlink™ LE0595 PE
Borlink™ LE4201EHV PE
Borlink™ LE4201R PE
Borlink™ LE4212 PE
Borlink™ LE4244EHV PE
Borlink™ LE4244R PE
Borlink™ LE4244S PE
Borlink™ LE4253DC PE
Borlink™ LE7710 PE
Borlink™ LE8280 PE
Borlink™ LH4201R PE
Borlink™ LS4201R PE
Borlink™ LS4201S PE
Borlink™ LE0310-04 PE
Borlink™ LE0504 PE
Borlink™ LE0594 PE
Borlink™ LE0595-07 PE
Borlink™ LR4201R PE
Borlink™ LR4201S PE
Borlink™ LS4201EHV PE
Borlink™ LS4201H PE
Borlink™ LS4258DCE PE
Borlink™ LS4258DCS PE

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.