Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE 430BE - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE 430BE:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
SABIC® LLDPE 430BE is a butene linear low density polyethylene resin. The material, natural resin, is typically used for cast film applications, offering good mechanically properties, stiffness enhancement and furthermore enables to gain high line speeds. SABIC® LLDPE 430BE is provided with a dedicated anti oxidant package suitable for cast film extrusion with low gel levels. Applications Skin layers for non-cling stretch cast film, cast film side encapsulation, mid layer hygienic cast film and product to realize downgauging by stiffness enhancement. Film properties Properties are determined on 20 ?m cast stretch film produced on a 2 m commercial cast stretch line: melt temperature 270 °C, chill roll temperature 20 °C and line speed of 450 m/min. Processing conditions SABIC® LLDPE 430BE is extrudable with conventional cast film extrusion equipment. Minor machine modifications may be required for optimum use. Cast film melt temperatures 250 - 300 °C. This product is not intended for and must not be used in any pharmaceutical/medical applications.
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура размягчения по Вика, A 109 °C ISO 306
Оптические свойстваЗначениеЕдиницаСтандарт
Данные ASTM
Мутность 2.4 % ASTM D 1003
Свойства пленкиЗначениеЕдиницаСтандарт
Данные ISO
Сопротивление распространению раздира, поперечное 117 Н/мм ISO 6383-1
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.