Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin SE1GFN1 - Europe - (PPE+PS)-GF10 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin SE1GFN1 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
NORYL™ SE1GFN1 resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V1 at 1.5mm along with UL746C Outdoor Suitability rating of F1 and RTI 110C. NORYL SE1GFN1 exhibits high heat resistance, good dielectric strength, dimensional stability, hydrolytic stability, and very low moisture absorption. This material is an excellent candidate for appliance internals, indoor and outdoor electrical enclosures / housings / connectors.

UL Yellow Card Link E45329-306538
Технологические и физические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Показатель текучести расплава, ПТР 15 см³/10мин ISO 1133
Температура 280 °C -
Нагрузка 10 kg -
Механические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Модуль упругости при растяжении 4000 МПа ISO 527
Напряжение в точке текучести 75 МПа ISO 527
Удлинение в точке текучести 2.5 % ISO 527
Напряжение при разрыве 70 МПа ISO 527
Удлинение при разрыве 3 % ISO 527
Модуль упругости при изгибе 3000 МПа ISO 178
Ударная прочность по Шарпи, +23°C 30 кДж/м2 ISO 179/1eU
Ударная прочность по Шарпи, -30°C, 3mm 30 кДж/м2 ISO 179/1eU
Ударная прочность по Шарпи с надрезом, +23°C, 3mm 6 кДж/м2 ISO 179/1eA
Ударная прочность по Шарпи с надрезом, -30°C, 3mm 5 кДж/м2 ISO 179/1eA
Izod impact strength, +23°C, 4mm 25 кДж/м2 ISO 180/1U
Izod impact strength, -30°C, 4mm 25 кДж/м2 ISO 180/1U
Ударная прочность по Изоду с надрезом, +23°C, 4мм 7 кДж/м2 ISO 180/1A
Ударная прочность по Изоду с надрезом, -30°C, 4мм 6 кДж/м2 ISO 180/1A
Твердость по вдавленному шарику 100 МПа ISO 2039-1
Теплофизические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Температура размягчения по Вика, A 145 °C ISO 306
Температура размягчения по Вика, B 140 °C ISO 306
Температура размягчения по Вика, 120°C/h 50N 145 °C ISO 306
Класс горючести при толщине образца h V-1 класс IEC 60695-11-10
Толщина образца 0.8 мм -
Класс горючести 5V при толщине образца h 5VA класс IEC 60695-11-20
Толщина образца 2.5 мм -
Термопроводность 0.27 W/(m K) DIN 52616
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 мм -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (2) 2 мм -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 мм -
Электрические свойстваЗначениеЕдиницаСтандарт
Данные ISO
Относительная диэлектрическая проницаемость, 1МГц 2.7 - IEC 62631-2-1
Коэффициент диэлектрических потерь, 1 MГц 30 E-4 IEC 62631-2-1
Удельное объемное сопротивление 1E11 Ом*м IEC 62631-3-1
Удельное поверхностное сопротивление >1E15 Ом IEC 62631-3-2
Электрическая прочность 33 кВ/мм IEC 60243-1
Сравнительный показатель пробоя 250 - IEC 60112
Прочие свойстваЗначениеЕдиницаСтандарт
Водопоглощение 0.22 % Sim. to ISO 62
Поглощение влаги 0.07 % Sim. to ISO 62
Плотность 1170 кг/м³ ISO 1183
Плотность 1160 кг/м³ ASTM D 792
Рекомендации по переработке литьем под давлениемЗначениеЕдиницаСтандарт
Температура предварительной сушки 100 - 120 °C -
Время предварительной сушки 2 - 3 h -
Температура расплава 280 - 300 °C -
Температура формы 80 - 120 °C -
Температура подачи 60 - 80 °C -
Зоны 1 240 - 260 °C -
Зоны 2 260 - 280 °C -
Зоны 3 280 - 300 °C -
Особые свойства и характеристики
Способы переработки
Литье под давлением
Добавки
Антипирен
Особые показатели
Огнестойкий
Химическая стойкость
Гидролитически устойчивый
Применение
Автомобилестроение
Доступность материала по регионам
Европа
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com