Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ PPE 646 - Europe - PPE - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ PPE 646 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Любая форма использования представленной информации должна осуществляться на основании заявленных условий и с учетом отсутствия ответственности создателей системы.
Описание продукта
NORYL™ PPE 646 resin is a high molecular weight polymer based on Polyphenylene Ether (PPE). This material is intended for use as an additive or a building block in a variety of thermoplastics and thermoplastic elastomers such as Styrenic Block Copolymers. PPE powder can be used to improve properties (i.e. Heat Distortion and Creep Resistance). It is hydrolytically stable and non-hydroscopic (typically less than 0.2% water uptake). The polymer is soluble in common organic solvents like toluene, chloroform, and THF. Chemical name: Poly (2,6-dimethyl-, 1,4-phenylene ether) (PPE) Formula: (C8H8O)n Regulatory Status: Complies with the FDA regulation 21CFR 177..2460. Also complies with EU Directive 2002/72/EC.
Прочие свойстваЗначениеЕдиницаСтандарт
Внутренняя вязкость 0.46 dl/g -
насыпная плотность 465 кг/м³ -
Особые свойства и характеристики
Сертификаты
Контакт с пищей, Одобрен для контакта с пищей FDA 21 CFR
Доступность материала по регионам
Европа
Дискламация
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Создан: Источник: www.materialdatacenter.com