Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PP PCGR40L - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PP PCGR40L:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
SABIC® PP grades for healthcare applications are produced under controlled conditions resulting in high product quality, consistency and a high level of purity. SABIC® PP PCGR40L is a highly transparent polypropylene random copolymer with good antistatic properties. This grade combines improved aesthetics of the finished articles with low temperature processability and a very good organoleptic performance. Part aesthetics are not affected by the lower temperatures, providing for a broader operating window, enabling short cycle times. SABIC® PP PCGR40L results in excellent demoulding characteristics and has a good stiffness to impact ratio. Typical applications: SABIC® PP PCGR40L is typically used for injection moulding of housings for empty disposable 2-part syringes. A lubrication agent is added to reduce friction between moving parts. Other applications demanding a high level of transparency and friction optimization are also possible. Compliance to regulations: SABIC® PP PCGR40L complies with the food contact regulations and the relevant monographs of the US Pharmacopoeia.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 1150 MPa ISO 527
Tensão no escoamento 29 MPa ISO 527
Deformação no escoamento 13 % ISO 527
Res. impacto Charpy c/entalhe, +23°C 4.5 kJ/m² ISO 179/1eA
Características
Processamento
Moldagem por injeção
Características especiais
Transparente
Características
Copolímero
Certifications
Contacto com alimentos
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.