Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP PCGR25 - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP PCGR25:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Informação do produto
SABIC® PP grades for healthcare applicationsare produced under controlled conditions resulting in high product quality, consistency and a high level of purity.
SABIC® PP PCGR25 is a highly transparent polypropylene random copolymer with good antistatic properties. This grade combines improved aesthetics of the finished articles with low melt temperature processability, enabling short cycle times. SABIC® PP PCGR25 results in good demoulding characteristics and has a good stiffness to impact ratio.
Typical applications: SABIC® PP PCGR25 has been typically designed for injection moulding of housings for empty disposable 3-part syringes. Others applications demanding a high level of transparency and broad processing window are also possible.
Compliance to regulations: SABIC® PP PCGR25 complies with the food contact regulations and the relevant monographs of theUS Pharmacopoeia. The product mentioned herein may not be used for medical healthcare devices or materials intended for temporary or permanent implementation in the human body.
IMDS 80775790
Propriedades mecânicas | Valor | Unidade | Método de ensaio |
ISO Dados |
Módulo de tração |
1050 |
MPa |
ISO 527 |
Tensão no escoamento |
25 |
MPa |
ISO 527 |
Deformação no escoamento |
13 |
% |
ISO 527 |
Res. impacto Charpy c/entalhe, +23°C |
6 |
kJ/m² |
ISO 179/1eA |
Características
Processamento
Moldagem por injeção
Características especiais
Transparente
Características
Copolímero
Certifications
Contacto com alimentos
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.