Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PP FPH50 - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PP FPH50:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
SABIC® PP FPH50 is a grade developed for thin wall packaging as well as the caps & closures market. The grade is nucleated and is characterised by a high crystallisation temperature, excellent flow behaviour in combination with a high stiffness. SABIC® PP FPH50 allows for very cost efficient processing on the basis of easy mould filling, very shortcycle times and robust processing behaviour in combination with pigments. It has a very good antistatic performance and shows easy demoulding. Application: SABIC® PP FPH50 is typically used in thin wall packing applications both for food and non-food segments. In caps and closure, the grade could be used for wide mouth caps, amongst others. In media packaging, the grade offers opportunities for cycle time optimisation. The grade has excellent heat deflection temperature making it particularly suitable for hot fill applications. Health, Safety and Food Contact regulations: Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site http://www.sabic.com. This product is not intended for and must not be used in any pharmaceutical/medical applications. This grade material is UL registered under File E111275 (www.ul.com) / IMDS 7172624
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2050 MPa ISO 527
Tensão no escoamento 39 MPa ISO 527
Deformação no escoamento 7 % ISO 527
Res. impacto Charpy c/entalhe, +23°C 3 kJ/m² ISO 179/1eA
Dureza Shore D 71 - ISO 7619-1
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 60 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 105 °C ISO 75-1/-2
Temperatura de amolecimento Vicat , A 154 °C ISO 306
Temperatura de amolecimento Vicat, B 103 °C ISO 306
Características
Certifications
Contacto com alimentos
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com