Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADITECK P RV400K 1700 NT - PPS-GF40 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADITECK P RV400K 1700 NT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Raditeck datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
PPS 40% glass fibre reinforced injection moulding grade. Heat stabilized. Natural colour.

Balanced matching of excellent chemical resistance, inherent flame retardancy and very good heat ageing properties retention. Suitable for parts requiring very high stiffness and high mechanical strength.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Contração após a moldagem, paralelo 0.1 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.6 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 14600 MPa ISO 527
Tensão na ruptura 195 MPa ISO 527
Deformação na ruptura 1.8 % ISO 527
Resistência ao impacto Charpy , +23°C 50 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 10 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 280 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 265 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 270 °C ISO 75-1/-2
Coef. de expansão térmica linear, paralelo 16 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 46 E-6/K ISO 11359-1/-2
Cartão Amarelo (yellow card) disponível sim - -
Flamabilidade a espessura h V-0 class IEC 60695-11-10
Espessuras do tubo de teste 0.8 mm -
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Índice comparativo de linha de fuga 125 - IEC 60112
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1630 kg/m³ ISO 1183
Diagrama
Tensão - deformação , RADITECK P RV400K 1700 NT, PPS-GF40, RadiciGroup
Módulo secante - deformação , RADITECK P RV400K 1700 NT, PPS-GF40, RadiciGroup
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulado, Cor natural
Aditivos
Desmoldante
Características especiais
Retardante de chama, Estável contra o calor
Resistência Química
Resistência química geral
Disponibilidade regional
Outras informações
Moldagem por injeção
The material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.05%. Typical conditions with a desiccant drier: temperature 115° C, dew point -20°C or below, time 3-4h or more. Avoid excessive shear rates and high thermal stresses for better processing. Special care must be taken to avoid moisture absorption and contamination with other polymers when adding regrind material. Colour variation and mechanical properties reduction may occur and should always be carefully monitored.

Injection Molding Processing Parameters
Melt TemperatureMold TemperatureInjection Speed
300 - 340°C140 - 160°Clow-medium
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.