Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin GFN2 - Americas - (PPE+PS)-GF20 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin GFN2 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
NORYL™ GFN2 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This general-purpose injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN2 carries a UL746C outdoor suitability rating of F1 and is an excellent candidate for a variety of indoor and outdoor applications including construction, electrical components + displays, lawn and garden equipment. *See NORYL GFN2F resin for FDA food compliant / NSF version.

UL Yellow Card Link E121562-221161
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 8 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 5 kg -
ASTM Dados
Índice de fluidez, MFI 9 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 5 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 7070 MPa ISO 527
Tensão na ruptura 97 MPa ISO 527
Deformação na ruptura 2.5 % ISO 527
Módulo de flexão 6540 MPa ISO 178
Res. impacto Izod c/entalhe, +23°C, 4mm 11 kJ/m² ISO 180/1A
ASTM Dados
Módulo de tração 6200 MPa ASTM D 638
Resistência à tração na ruptura 90 MPa ASTM D 638
Deformação na ruptura 2.6 % ASTM D 638
Módulo de flexão 5800 MPa ASTM D 790
Dureza Rockwell L106 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 119 J/m ASTM D 256
Impacto Izod com entalhe, baixa temperatura 96 J/m ASTM D 256
Temperatura -40 °C -
Resistência ao Impacto Izod, 1/8 in 650 J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de amolecimento Vicat, B 143 °C ISO 306
Temperatura de amolecimento Vicat, 120°C/h 50N 146 °C ISO 306
Coeff. of linear therm. expansion -40°C to +100°C, parallel 3.3E-5 E-6/K ISO 11359-1/-2
Coeff. of linear therm. expansion -40°C to +100°C, normal 9.0E-5 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.5 mm -
ASTM Dados
DTUL @ 66 psi 140 °C ASTM D 648
DTUL @ 264 psi 135 °C ASTM D 648
Propriedades elétricasValorUnidadeMétodo de ensaio
ASTM Dados
Resistência elétrica, tempo curto 16.5 kV/mm ASTM D 149
Fator de dissipação dielétrica, 60 Hz 0.0008 - ASTM D 150
Constante dielétrica, 60 Hz 2.86 - ASTM D 150
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1200 kg/m³ ASTM D 792
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 110 - 120 °C -
Pré-secagem - tempo 3 - 4 h -
Umidade do processamento ≤0.02 % -
Temperatura da massa 300 - 325 °C -
Temperatura do molde 80 - 110 °C -
Zona 1 265 - 315 °C -
Zona 2 275 - 320 °C -
Zona 3 290 - 325 °C -
Velocidade de parafuso 20 - 100 rpm -
Contrapressão 0.3 - 0.7 MPa -
Características
Processamento
Moldagem por injeção
Resistência Química
Estabilidade hidrolítica
Certifications
Contacto com alimentos, Aprovação de alimentos FDA 21 CFR
Aplicaciones
Automóvel
Disponibilidade regional
América do Norte
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com