Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® Vestolen P 9421 - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® Vestolen P 9421:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Informação do produto
This random copolymer has a high molecular weight with special designed properties required for high demandingpressure pipes. It is highly heat stabilised and especially formulated for extraction resistance. This grade with long service life is used for the manufacturing of cold and hot water pipes and fittings for transport of drinking water. This grade fulfills the requirements in EN ISO 15874, ISO 3213, DIN 8078 and DIN 8077. It also complies with German regulations for materials in contact with water intended for human consumption (BGA requirements and KTW recommendations). Health, Safety and Food Contact regulations:Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site
http://www.SABIC-europe.comThe product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.IMDS 80775790
Propriedades mecânicas | Valor | Unidade | Método de ensaio |
ISO Dados |
Módulo de tração |
900 |
MPa |
ISO 527 |
Tensão no escoamento |
28 |
MPa |
ISO 527 |
Deformação no escoamento |
13 |
% |
ISO 527 |
Resistência ao impacto Charpy, +23°C |
N |
kJ/m² |
ISO 179/1eU |
Dureza Shore D |
63 |
- |
ISO 7619-1 |
Propriedades térmicas | Valor | Unidade | Método de ensaio |
ISO Dados |
Temperatura de amolecimento Vicat , A |
129 |
°C |
ISO 306 |
Temperatura de amolecimento Vicat, B |
68 |
°C |
ISO 306 |
Características
Características especiais
Estável contra o calor
Características
Copolímero
Certifications
Contacto com alimentos, Contato com água potável, Contato com água potável KTW
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.