Material datasheets available free. Online registration at: www.materialdatacenter.com
Latiohm - ABS, PA6, PA66, PBT, PC, PESU, POM, PPA, PPS - LATI Industria Termoplastici S.p.A
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Latiohm" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
LATIOHM 36/07 PD01 G/20 | ABS-GF |
LATIOHM 52/11-10 PD02 | PP |
LATIOHM 62-03 PD01 G/20 | PA6-GF |
LATIOHM 62-08 PD02 G/30 | PA6-GF |
LATIOHM 62-09 PD01 G/20-V2HF | PA6-GF |
LATIOHM 63-08 PD02 G/25 | PA6-GF |
LATIOHM 66-04 PD01 G/25-V0CT1 | PA66-GF |
LATIOHM 66-05 PD01 G/20 | PA66-GF |
LATIOHM 66-06 PD03 G/20 | PA66-GF |
LATIOHM 66-08 PD02 G/35 | PA66-GF |
LATIOHM 66-10 H2 CNT CE/10 | PA66-(MX+Z) |
LATIOHM 66-10 H2 CNT G/35 | PA66-(GF+Z) |
LATIOHM 73-09 PD01 G/20 | POM-GF |
LATIOHM 73/23-10 CNT | POM-Z |
LATIOHM 75/4-03 PD01 G/20 | PBT-GF |
LATIOHM 75/4-10 CNT | PBT-Z |
LATIOHM 80-04 PD01 G/30 | PPS-GF |
LATIOHM 80-05 CNT GCE/500 | PPS-(GF+MX) |
LATIOHM 85-06 PD01 G/15 | PESU-GF |
LATIOHM 87/28-05 PD01 G/10 | PC-GF |
LATIOHM 87/28-07 CNT | PC-Z |
LATIOHM 88/10-06 CNT | PEEK-Z |
LATIOHM 90/13-09 PD01 G/10 | PPO-GF |
LATIOHM 57-05 PD01 G/15 | PPA-GF |
LATIOHM 66-07 PD08 G/30 | PA66-GF |
LATIOHM 75/4-08 PD01 G/30 | PBT-GF |
LATIOHM 82-02 PD09 | PA12 |
LATIOHM 83-07 PD11 CNT | PA12-Z |
LATIOHM 87/26-06 PD01-V1 | PC |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.