Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint™ TPU 88A - TPU - BASF

Material Data Center offers the following functions for Ultrasint™ TPU 88A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
기계적 특성단위시험규격
ISO 데이터
쇼어 A 경도 89 - ISO 7619-1
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 135 °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min -48 °C ISO 11357-1/-2
기타 특성단위시험규격
밀도 1100 kg/m³ ISO 1183
Bulk density 500 kg/m³ -
3D Data단위시험규격
Other Standards[S]
인장탄성률, flat 75 MPa ISO 527
인장탄성률, upright 75 MPa ISO 527
인장 강도, flat 8 MPa ISO 527
인장 강도, upright 7 MPa ISO 527
파단시 신율 , flat 270 % ISO 527
파단시 신율 , upright 130 % ISO 527
굴곡 계수, flat 70 MPa ISO 178
굴곡 계수, upright 70 MPa ISO 178
챠피 노치드 충격 강도, +23°C, flat 0 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, +23°C, upright 0 kJ/m² ISO 179/1eA
비카트 연화 온도, A, flat 98 °C ISO 306
비카트 연화 온도, A, upright 98 °C ISO 306
S: These properties are reported by the producer according standards that are different to our defaults.
특징
생산 공정
Additive Manufacturing, Laser Sintering
인도 유형
가루, 화이트
특별 특성
U.V. 안정성 또는 기후 안정성
내화학성에
Hydrolytically Stable
응용
스포츠 장비
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.