Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of ULTEM™ Resin 2312 - Americas - PEI-GF30 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for ULTEM™ Resin 2312 - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Ultem datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.

UL Yellow Card Link E121562-221100
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 열전도율 0.3 W/(m K) -
용융 비열용량 1920 J/(kg K) -
이형온도 208 °C -
ASTM 데이터
용융 흐름성, MFI 10.1 g/10min ASTM D 1238
온도 337 °C -
하중 6.6 kg -
기계적 특성단위시험규격
ASTM 데이터
인장탄성률 5990 MPa ASTM D 638
파단시 강도 103 MPa ASTM D 638
파단시 신율 3.5 % ASTM D 638
아이조드 충격은 노치, 1/8 in 32 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
선형 열팽창 계수, 평행 27.3 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 33.4 E-6/K ISO 11359-1/-2
두께 H인 제품의 난연성 V-0 class IEC 60695-11-10
테스트 두께 0.8 mm -
전기적 특성단위시험규격
ASTM 데이터
상대 유전율, 1 MHz 3.49 - ASTM D 150
기타 특성단위시험규격
밀도 1510 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 150 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
용융수지온도 350 - 400 °C -
성형온도 135 - 165 °C -
Zone 1 330 - 400 °C -
Zone 2 340 - 400 °C -
Zone 3 345 - 400 °C -
Screw speed 40 - 70 rpm -
Back pressure 0.3 - 0.7 MPa -
도표
점도-변형률 , ULTEM™  Resin 2312 - Americas, PEI-GF30, SABIC
전단-변형률 , ULTEM™  Resin 2312 - Americas, PEI-GF30, SABIC
비용적-온도(pvT) , ULTEM™  Resin 2312 - Americas, PEI-GF30, SABIC
특징
생산 공정
사출 성형
응용
자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.