Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LDPE 2201H1W - (PE-LD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LDPE 2201H1W:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
SABIC® LDPE 2201H1W is a grade with a low level of anti block and a medium level of slip agent. The grade has a very good draw down ability. Films based on 2201H1W combine toughness with high tear strength, good optical properties and low CoF. Application SABIC® LDPE 2201H1W is typically used for lamination films, high quality carrier bags and high quality packaging films. SABIC® LDPE 2201H1W can typically be used for food applications due to very low migration levels. Film properties Film properties have been measured at film of 50 ?m with a BUR of 3. The film has been produced on Kiefel IBC blown film line with 200 kg/h. Die size 200 mm, die gap 0.8 mm. This product is not intended for and must not be used in any pharmaceutical/medical applications.
광학 특성단위시험규격
ASTM 데이터
탁도 6 % ASTM D 1003
기계적 성질 (필름) 단위시험규격
ISO 데이터
인장탄성률, 수직 170 MPa ISO 527-3
항복시의 강도, normal 11 MPa ISO 527-3
파단시 강도, 평행 25 MPa ISO 527-3
파단시 강도, 수직 20 MPa ISO 527-3
트라우저 전단강도, 평행 45 N/mm ISO 6383-1
트라우저 전단강도, 수직 45 N/mm ISO 6383-1
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.