Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilon F 50 natural 6368 - PA6 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilon F 50 natural 6368:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Grilon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Product-nomenclature: ISO 16396-PA6,,F,S34-030N

 

Product Attributes

  High viscosity, Barrier material

Markets

  Industry & Consumer goods
  Mechanical Engineering
  Packaging
  Blow moulded containers, Injectionstretchblowmoulded containers

Approvals

  Food Contact
  EU Requirements, FDA
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 45 / * cm³/10min ISO 1133
온도 275 / * °C -
하중 21.6 / * kg -
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 - / 750 MPa ISO 527
챠피 노치드 충격 강도, -30°C - / 5 kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 222 / * °C ISO 11357-1/-3
광학 특성건조/응축단위시험규격
ISO Data
광택도, 60° 100 / * - ISO 2813
기타 특성건조/응축단위시험규격
물에서의 흡수성 9 / * % ISO 62와 유사
조건에서의 흡습성 3 / * % ISO 62와 유사
밀도 1140 / - kg/m³ ISO 1183
기계적 성질 (필름) 건조/응축단위시험규격
ISO 데이터
항복시의 강도, 평행 35 / * MPa ISO 527-3
항복시의 강도, 수직 30 / * MPa ISO 527-3
항복시의 변형율, 평행 15 / * % ISO 527-3
항복시의 변형율, 수직 15 / * % ISO 527-3
최대변형율, 평행 700 / * % ISO 527-3
최대변형율, 수직 700 / * % ISO 527-3
엘멘도프 전단강도, 평행 10 / * N ISO 6383-2
엘멘도프 전단강도, 수직 10 / * N ISO 6383-2
트라우저 전단강도, 평행 30 / * N/mm ISO 6383-1
트라우저 전단강도, 수직 30 / * N/mm ISO 6383-1
수증기 투과속도, 23°C/85%RH 15 / * g/(m²*d) ISO 15106-1/-2
산소 투과율, 23°C/0%r.h. 25 / * cm³/(m²*d*bar) ISO 15105-1/-2
산소 투과율, 23°C/85%RH 50 / * cm³/(m²*d*bar) ISO 15105-1/-2
이산화탄소 투과율, 23°C/0%r.h. 80 / * cm³/(m²*d*bar) ISO 15105-1/-2
이산화탄소 투과율, 23°C/85%RH 250 / * cm³/(m²*d*bar) ISO 15105-1/-2
특징
생산 공정
외형 압출, 시트 압출, 기타 압출, 중공 성형
인도 유형
과립, 자연 색상
특성
Barrier Properties
Certifications
Food contact, Food approval FDA 21 CFR
응용
포장
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.