Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ GR2300 - PA9T-GF30 FR - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ GR2300:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Genestar GR2300 is one of standard grades.

Main feature of GR2300 is;:
 -Good balance of mechanical strength, mold ability, and dimensional stability

Examples of applications are:
 -FPC Connectors
 -Board to Board / Wire to Board Connectors
Processing/Physical Characteristics단위시험규격
ISO 데이터
성형 수축률, 평행 0.2 % ISO 294-4, 2577
성형 수축률, 수직 0.8 % ISO 294-4, 2577
ASTM 데이터
용융 흐름성, MFI 16 g/10min ASTM D 1238
온도 320 °C -
하중 2.16 kg -
기계적 특성단위시험규격
ISO 데이터
인장 강도 175 MPa ISO 527
파단시 강도 175 MPa ISO 527
파단시 신율 2 % ISO 527
굴곡 계수, 23°C 10800 MPa ISO 178
굴곡 강도 239 MPa ISO 178
챠피 노치드 충격 강도, +23°C 10 kJ/m² ISO 179/1eA
ASTM 데이터
인장 강도 180 MPa ASTM D 638
굴곡 계수 10000 MPa ASTM D 790
굴곡 강도 220 MPa ASTM D 790
아이조드 충격은 노치, 1/8 in 100 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 306 °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 125 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 285 °C ISO 75-1/-2
두께 H인 제품의 난연성 V-0 class IEC 60695-11-10
ASTM 데이터
UL94 난연성 V-0 - UL 94
DTUL @ 264 psi 285 °C ASTM D 648
녹는점 306 °C ASTM D 3418
유리 전이 온도 125 °C ASTM E 1356
전기적 특성단위시험규격
ASTM 데이터
전기 압력, 단기간의 30 kV/mm ASTM D 149
부피 저항 >1E15 Ohm*cm ASTM D 257
기타 특성단위시험규격
물에서의 흡수성 0.14 % ISO 62와 유사
밀도 1570 kg/m³ ISO 1183
밀도 1570 kg/m³ ASTM D 792
도표
응력-신율 , Genestar™ GR2300, PA9T-GF30 FR, Kuraray
시컨트탄성율-신율 , Genestar™ GR2300, PA9T-GF30 FR, Kuraray
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com