Tecotek - PC - Eurotec Mühendislik Plastikleri
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Tecotek" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
Tecotek® BC40 UF45 NL CE | (PC+ABS) |
Tecotek® BC40 UF65 NL CE | (PC+ABS) |
Tecotek® BC40 UF85 NL CE | (PC+ABS) |
Tecotek® BC43 UF65 NL CE | (PC+ABS) |
Tecotek® PC30 GR20 GR003 ZG20 | PC-GF20 |
Tecotek® PC30 NL RX | PC |
Tecotek® PC30 NL TD70 | PC |
Tecotek® PC30 NL VB03 | (PC+PET) |
Tecotek® PC40 GR10 NL | PC-GF10 |
Tecotek® PC40 GR20 NL | PC-GF20 |
Tecotek® PC40 GR30 NL | PC-GF30 |
Tecotek® PC40 NL FA70 | PC |
Tecotek® PC40 NL VB02 | (PC+PBT) |
Tecotek® PC43 GR003 TD70 | PC |
Tecotek® PC43 GR10 BK002 | PC-GF10 |
Tecotek® PC43 GR20 BK002 | PC-GF20 |
Tecotek® PC43 GR30 BK002 | PC-GF30 |
Tecotek® PC44 GR003 ZG70 | PC |
Tecotek® PC44 GR10 GR003 ZG70 | PC-GF10 |
Tecotek® PC50 GR10 GR053 FA20 | PC-GF10 |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.