Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP 520P - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP 520P:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
제품 설명서
SABIC® PP 520P is particularly designed for extrusion of cast film, both mono layer films and co extruded films. It provides an excellent combination of transparency, stiffness and high heat resistance. SABIC® PP 522L is the anti block and slip agent containing version of SABIC® PP 520P.Application:SABIC® PP 520P is typically used for food packaging, lamination film, stationary film, textile packaging, flower packaging, and hygiene packaging. It offers excellent properties for twist film application. Health, Safety and Food Contact regulations: SABIC® PP 520P has a Food Contact Declaration. SABIC Material Safety Data Sheets (MSDS) and Product Safety Declarations are available on our Internet site
http://www.sabic.com.The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications.This grade material is UL registered under File E111275 (www.ul.com)IMDS 7172624
기계적 특성 | 값 | 단위 | 시험규격 |
ISO 데이터 |
인장탄성률 |
1700 |
MPa |
ISO 527 |
항복강도 |
36 |
MPa |
ISO 527 |
항복변형률 |
9 |
% |
ISO 527 |
열적 특성 | 값 | 단위 | 시험규격 |
ISO 데이터 |
비카트 연화 온도, A |
154 |
°C |
ISO 306 |
비카트 연화 온도, B |
95 |
°C |
ISO 306 |
특징
Certifications
Food contact
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.