Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of Deltron 5311 - PPS-CF - Lingen Plastic Rubber Co., Ltd.
Material Data Center offers the following functions for Deltron 5311:
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Deltron datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
Processing/Physical Characteristics | 값 | 단위 | 시험규격 |
Other Standards[S] |
성형 수축률, 평행 |
0.002 |
mm/mm |
|
성형 수축률, 수직 |
0.005 |
mm/mm |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
기계적 특성 | 값 | 단위 | 시험규격 |
Other Standards[S] |
인장 강도 |
140 |
MPa |
|
압축 강도 |
140 |
MPa |
|
굴곡 계수 |
17000 |
MPa |
|
굴곡 강도 |
210 |
MPa |
|
로크웰 경도 |
R 110 |
- |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
열적 특성 | 값 | 단위 | 시험규격 |
ASTM 데이터 |
UL94 난연성 |
V-0 |
- |
UL 94 |
테스트 두께 |
2 |
mm |
- |
Other Standards[S] |
열팽창 계수, 평행 |
18 |
E-6/K |
|
DTUL @ 264 psi |
265 |
°C |
|
녹는점 |
285 |
°C |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
전기적 특성 | 값 | 단위 | 시험규격 |
Other Standards[S] |
표면 저항 |
1E10 |
Ohm |
|
부피 저항 |
1E11 |
Ohm*cm |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
기타 특성 | 값 | 단위 | 시험규격 |
Other Standards[S] |
밀도 |
1700 |
kg/m³ |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
특징
특별 특성
정전기 방지
지역별 검색
쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.