Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrasint PA11 GB30 - PA11-GB30 - BASF

Material Data Center offers the following functions for Ultrasint PA11 GB30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrasint datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics乾燥/調湿単位テスト基準
ISO データ
メルトボリュームレイト, MVR 10 / * cm³/10min ISO 1133
温度 220 / * °C -
荷重 2.16 / * kg -
熱的特性乾燥/調湿単位テスト基準
ISO データ
溶融温度, 10゚C/min 203 / * °C ISO 11357-1/-3
荷重たわみ温度, 1.80 MPa 87 / * °C ISO 75-1/-2
荷重たわみ温度, 0.45 MPa 176 / * °C ISO 75-1/-2
ビカット軟化温度, A 192 / * °C ISO 306
ビカット軟化温度, B 171 / * °C ISO 306
その他の特性.乾燥/調湿単位テスト基準
密度. 1240 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
3D Data乾燥/調湿単位テスト基準
Other Standards[S]
引張弾性率, flat 2600 / 1200 MPa ISO 527
引張弾性率, upright 2500 / 1200 MPa ISO 527
引張強度, flat 47 / 33 MPa ISO 527
引張強度, upright 45 / 32 MPa ISO 527
破壊ひずみ, flat 7 / 66 % ISO 527
破壊ひずみ, upright 4 / 34 % ISO 527
曲げ弾性率, flat 2550 / 1450 MPa ISO 178
曲げ弾性率, upright 2450 / 1400 MPa ISO 178
シャルピー衝撃強さ, +23°C, flat 40 / 166 kJ/m² ISO 179/1eU
シャルピー衝撃強さ, +23°C, upright 25 / 63 kJ/m² ISO 179/1eU
ノッチ付きシャルピー衝撃強さ, +23°C, flat 6.3 / 13 kJ/m² ISO 179/1eA
ノッチ付きシャルピー衝撃強さ, +23°C, upright 5.7 / 10 kJ/m² ISO 179/1eA
アイゾット衝撃試験, +23°C, flat 32 / 0 kJ/m² ISO 180/1U
アイゾット衝撃試験, +23°C, upright 20 / 51 kJ/m² ISO 180/1U
ノッチ付きIzod衝撃強さ, +23°C, flat 6.8 / 16 kJ/m² ISO 180/1A
ノッチ付きIzod衝撃強さ, +23°C, upright 5.9 / 11 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
特殊な特性
成形加工法.
Additive Manufacturing, Laser Sintering
納入形状.
パウダー., ナチュラルカラー
特殊な特性.
高耐衝撃及び耐衝撃改良.
な特性
Ductile, Thermal Stability
耐薬品性
General Chemical Resistance, Oil Resistance
Certifications
Contains renewable resources
アプリケーション
自動車
領域別の利用可能性
ヨーロッパ.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.