Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PPcompound 5040 - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PPcompound 5040:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
SABIC® PPcompound 5040 is an impact-modified Polypropylene for automotive interior applications. This material is emission optimized and has been designed to combine a good performance profile with good processing. SABIC® PPcompound 5040 is a designated automotive grade. IMDS ID: 666993041
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトフローレート, MFI 30 g/10min ISO 1133
温度 230 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 1450 MPa ISO 527
降伏応力 25 MPa ISO 527
破壊応力 16 MPa ISO 527
破壊ひずみ 25 % ISO 527
曲げ弾性率, 23°C 1500 MPa ISO 178
ノッチ付きIzod衝撃強さ 4 kJ/m² ISO 180/1A
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 0.45 MPa 90 °C ISO 75-1/-2
その他の特性.単位テスト基準
密度. 905 kg/m³ ISO 1183
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.