Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of SABIC® PP QR673K - PP - Saudi Basic Industries Corporation (SABIC)
Material Data Center offers the following functions for SABIC® PP QR673K:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces
Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center
Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our
disclaimer.
商品の説明文
SABIC® PP QR673K is a highly transparent random copolymer with good antistatic properties. This grade combines improved aesthetics of the finished articles with low temperature processability. Part aesthetics are not affected by the lower temperatures, providing for a broader operating window. The SABIC® PP QR673K results in excellent demoulding characteristics and has a good stiffness to impact ratio.Application: SABIC® PP QR673K is mainly used in injection moulding processes. The SABIC® PP QR673K aims at transparent applications ranging from injection moulded housewares, office & home storage boxes, lids to caps & closures.Health, Safety and Food Contact regulations: Material Safety Data Sheets (MSDS) and Product Safety declarations are available on our Internet site
http://www.SABIC.comThe product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/ medical applications. This grade material is UL registered under File E111275 (www.ul.com) / IMDS 80775790
機械的特性 | 値 | 単位 | テスト基準 |
ISO データ |
引張弾性率 |
1050 |
MPa |
ISO 527 |
降伏応力 |
25 |
MPa |
ISO 527 |
降伏ひずみ |
13 |
% |
ISO 527 |
ノッチ付きシャルピー衝撃強さ, +23°C |
6 |
kJ/m² |
ISO 179/1eA |
ショア硬さD |
62 |
- |
ISO 7619-1 |
熱的特性 | 値 | 単位 | テスト基準 |
ISO データ |
荷重たわみ温度, 1.80 MPa |
50 |
°C |
ISO 75-1/-2 |
荷重たわみ温度, 0.45 MPa |
75 |
°C |
ISO 75-1/-2 |
ビカット軟化温度, A |
125 |
°C |
ISO 306 |
ビカット軟化温度, B |
68 |
°C |
ISO 306 |
特殊な特性
成形加工法.
射出成形.
特殊な特性.
透明.
な特性
Copolymer
Certifications
Food contact
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com
Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.
Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.