Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE M500026 - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE M500026:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
M500026 is a Linear Low Density Polyethylene grade with narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excellent flow properties with better low temperature toughness, stress crack resistance and gloss.
Processing/Physical Characteristics単位テスト基準
ASTM数据
メルトフローレイト, MFI 50 g/10min ASTM D 1238
温度 190 °C -
荷重 2.16 kg -
機械的特性単位テスト基準
ISO データ
ショア硬さD 55 - ISO 7619-1
ASTM数据
降伏応力 13 MPa ASTM D 638
破壊応力 12.4 MPa ASTM D 638
破断伸び 120 % ASTM D 638
曲げ弾性率 200 MPa ASTM D 790
曲げ強さ 9 MPa ASTM D 790
ショア硬さD 50 - ASTM D 2240
アイゾット衝撃試験, 1/8 in 500 J/m ASTM D 256
熱的特性単位テスト基準
ASTM数据
ビカット軟化温度 88 °C ASTM D 1525
特殊な特性
成形加工法.
射出成形.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.