Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LDPE Powder 1965P9 - (PE-LD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LDPE Powder 1965P9:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
SABIC® LDPE Powder 1965P9 is an additive free standard CTR® tubular grade for masterbatch with a typically low viscosity. This grade has a typically high filler acceptance. Application SABIC® LDPE Powder 1965P9 is a normal sized powder grade. Since the grade is supplied in powder form it is typically suited for pre mixing. The flow and dispersion of pigments and additives that tend towards blocking are typically improved by adding this grade. This product is not intended for and must not be used in any pharmaceutical/medical applications.
熱的特性単位テスト基準
ISO データ
ビカット軟化温度, A 75 °C ISO 306
その他の特性.単位テスト基準
Bulk density 330 kg/m³ -
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.