Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kepstan® 6001 - PAEK - ARKEMA

Material Data Center offers the following functions for Kepstan® 6001:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kepstan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
KEPSTAN® PEKK resin is a high performance thermoplastic material, based on PolyEtherKetoneKetone (PEKK) highly stable chemical backbone. KEPSTAN® PEKK is a unique member of the PAEK family that incorporates distinctive structural features that allow for exceptional possibilities in the control of crystallinity. These features include a low Ether/Ketone ratio and a copolymer structure incorporating Terephtalic and Isophtalic moieties.

The 6000 Series represents the pseudo-amorphous products of the KEPSTAN® family, offering the lowest melting point and the slowest crystallization behavior, while keeping Tg close to 160°C. These properties allow for lower processing temperatures (as low as 320-330°C), and lead to glassy or semi crystalline structures, depending on processing technologies and cooling conditions.

KEPSTAN® 6000 Series includes a medium flow grade, KEPSTAN® 6002, and a high flow grade, KEPSTAN® 6003, both unfilled PEKK resins designed to meet the requirements of a broad range of processing technologies, including among others extrusion, calendering, thermoforming, injection molding, fiber impregnation, rotomolding, powder coating, bonding and welding. 

KEPSTAN® PEKK resin is available in pellet form as well as in powder form with different particle sizes. Standard packaging includes 20 kg boxes for pellets and 10 kg boxes for powders.
Processing/Physical Characteristics単位テスト基準
ISO データ
メルトボリュームレイト, MVR 15 cm³/10min ISO 1133
温度 380 °C -
荷重 5 kg -
機械的特性単位テスト基準
ISO データ
引張弾性率 3100 MPa ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 5.1 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
荷重たわみ温度, 1.80 MPa 139 °C ISO 75-1/-2
酸素指数 38 % ISO 4589-1/-2
電気的特性.単位テスト基準
ISO データ
比誘電率, 1MHz 3 - IEC 62631-2-1
その他の特性.単位テスト基準
吸水率 1.07 % Sim. to ISO 62
吸湿率 0.44 % Sim. to ISO 62
密度 1270 kg/m³ ISO 1183
特殊な特性
成形加工法.
射出成形., 異形押出成形., シート押出成形., コーティング., ブロー成形., カレンダー加工., トランスファー成形., 熱成形.
納入形状.
ペレット.
領域別の利用可能性
その他の情報
村遜速揃
Drying temperature and time: 120°C for 6 to 8 hours
Processing temperature: 320 – 360°C
Temperature settings - Injection: Rear 300°C / Center 315°C / Front 320°C / Nozzle 330°C
Mold temperature (below Tg in any case): 80 - 120°C
Temperature settings - Extrusion:  Zones 1/2/3/4: 290°C/ 320°C/ 330°C/ 320°C   Die: 320°C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.