Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Genestar™ G1300A-M41 - PA9T-GF30 - Kuraray Co., Ltd.

Material Data Center offers the following functions for Genestar™ G1300A-M41:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Genestar datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
商品の説明文
G1300A-M41 (black, natural) is a standard 30% GF reinforced injection molding grade provided as pellets.

The main features are:
  • Performance at high temperature
  • Low water absorption and retention of its initial properties
  • Dimensional stability

This grade is suitable for:
  • Gears and bearing retainers
  • Parts in harsh chemical and thermal environments
Processing/Physical Characteristics単位テスト基準
ISO データ
成形収縮率, 平行 0.3 % ISO 294-4, 2577
成形収縮率, 直角 0.9 % ISO 294-4, 2577
機械的特性単位テスト基準
ISO データ
引張弾性率 9740 MPa ISO 527
破壊応力 190 MPa ISO 527
破壊ひずみ 2.5 % ISO 527
ノッチ付きシャルピー衝撃強さ, +23°C 10 kJ/m² ISO 179/1eA
熱的特性単位テスト基準
ISO データ
溶融温度, 10°C/min 300 °C ISO 11357-1/-3
ガラス転移点, 10°C/min 125 °C ISO 11357-1/-2
荷重たわみ温度, 1.80 MPa 270 °C ISO 75-1/-2
ASTM数据
線膨張係数, 平行 24 E-6/K ASTM D 696
線膨張係数, 直角 41 E-6/K ASTM D 696
その他の特性.単位テスト基準
吸水率 0.19 % Sim. to ISO 62
密度 1370 kg/m³ ISO 1183
機能
 応力-ひずみ. , Genestar™ G1300A-M41, PA9T-GF30, Kuraray
 割線弾性率−ひずみ. , Genestar™ G1300A-M41, PA9T-GF30, Kuraray
 pvT , Genestar™ G1300A-M41, PA9T-GF30, Kuraray
特殊な特性
成形加工法.
射出成形.
納入形状.
黒, ナチュラルカラー
添加剤.
離型剤.
特殊な特性.
熱安定化.
な特性
Barrier Properties, Creep Resistance, Fatigue Resistance, High Crystallinity, Thermal Stability, Weldable
耐薬品性
Acid Resistance, Alkali Resistance, General Chemical Resistance, Environmental Stress Crack Resistance, Solvent Resistance, Grease Resistance, Hydrolytically Stable, Oil Resistance
アプリケーション
自動車, 汎用
領域別の利用可能性
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.