Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of THERMOLAST® M TM7MED - TPE - KRAIBURG TPE GmbH & Co. KG
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Thermolast datasheets, application examples or technical articles are available in Material Data Center
• Medical application
Application Examples:
• Seals
• Mouthpieces
• Valves
• Soft touch
• Flexible connections
• Medical tubes
Material Advantage:
• Applicaton up to indirect blood contact
• Tested acord. USP Class IV and ISO 10993-5
• Tested according to ISO 10993-11, ISO 10993- 10, USP 6.6.1
• Adhesion to PP und HDPE
• Adapted for injection moulding and extrusion
• Very good compression set
• sterilizable (autoclave 134°C, gammaradiation 2x35 kGy, EtO)
機械的特性 | 値 | 単位 | テスト基準 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ISO データ | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
引張強度 | 13 | MPa | ISO 37 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
破壊ひずみ | 800 | % | ISO 37 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
圧縮永久ひずみ 70℃, 24h | 38 | % | ISO 815 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
圧縮永久ひずみ 100℃, 24h | 55 | % | ISO 815 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
引裂強さ | 23.5 | kN/m | ISO 34-1 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ショア硬さA | 68 | - | ISO 7619-1 |
その他の特性. | 値 | 単位 | テスト基準 |
密度. | 890 | kg/m³ | ISO 1183 |
Processing Recommendation Injection Molding | 値 | 単位 | テスト基準 |
Pre-drying - Temperature | 60 - 80 | °C | - |
Pre-drying - Time | 2 - 4 | h | - |
樹脂温度 | 200 - 250 | °C | - |
金型温度 | 25 - 40 | °C | - |
Zone 1 | 180 - 200 | °C | - |
Zone 2 | 200 - 220 | °C | - |
Zone 3 | 220 - 250 | °C | - |
Injection pressure | 20 - 100 | MPa | - |
Back pressure | 2 - 10 | MPa | - |
後硬化時間 | 8 - 60 | MPa | - |
Maximum residence time | 10 | min | - |