Radilon S - PA6 - RadiciGroup High Performance Polymers

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Radilon S" in Material Data Center leads to the following information:

Tradename: Radilon S
Family: PA6
Producer: RadiciGroup High Performance Polymers
41 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
RADILON S BF 990 GY PA6
RADILON S BMX200K 333 BK PA6
RADILON S CP300K 100 NT PA6-MD30
RADILON S CV300 100 NT PA6-GB30
RADILON S ERV100 FR2 333 BK PA6-GF10
RADILON S ESL128 100 NT PA6
RADILON S HS 105 M NT PA6
RADILON S HSX 100 NT PA6
RADILON S HSX88 100 NT PA6
RADILON S RCP4015LK 100 NT PA6-(GF+T)40
RADILON S RCV3015 100 NT PA6-(GF+GB)30
RADILON S RV150 100 NT PA6-GF15
RADILON S RV200 100 NT PA6-GF20
RADILON S RV200 FR2 100 NT PA6-GF20
RADILON S RV300 100 NT PA6-GF30
RADILON S RV300 FR2 100 NT PA6-GF30
RADILON S RV300W 333 BK PA6-GF30
RADILON S RV350W 333 BK PA6-GF35
RADILON S RV500K 333 BK PA6-GF50
RADILON S URV300W 333 BK PA6-GF30
RADILON S URV600W 339 BK PA6-GF60
RADILON S USX270 333 BK PA6
RADILON S USZ200 100 NT PA6
RADILON S RV250 100 NT PA6-GF25
RADILON S USX200 100 NT PA6
RADILON S BMV150K 333 BK PA6-GF15
RADILON S LERV150K 100 NT PA6-GF15
RADILON S LRV150UK 333 BK PA6-GF15
RADILON S RCP3010LW 322 BK PA6-(GF+T)30
RADILON S RCP4015LK 333 BK PA6-(GF+T)40
RADILON S RCW4015W 3733 BK PA6-(GF+MF)40
RADILON S RV150W 333 BK PA6-GF15
RADILON S RV250 FR2 5138 OR PA6-GF25
RADILON S RV300K 100 NT PA6-GF30
RADILON S RV350K 100 NT PA6-GF35
RADILON S RV350RG 1900 NT PA6-GF35
RADILON S RV350X2N 333 BK PA6-GF35
RADILON S RV400K 333 BK PA6-GF40
RADILON S RV500W 333 BK PA6-GF50
RADILON S RV500X2N 333 BK PA6-GF50
RADILON S URV500W 333 BK PA6-GF50

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.