Denyl HT - PPA - VAMP TECH SPA

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Denyl HT" in Material Data Center leads to the following information:

Tradename: Denyl HT
Family: PPA
Producer: VAMP TECH SPA
9 hits in the material database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Datasheet Polymer
Denyl HT 2010 PPA-GF20
Denyl HT 2010 Y (PPA+PA66)-GF20
Denyl HT 3510 PPA-GF35
Denyl HT 3510 Y (PPA+PA66)-GF35
Denyl HT 4010 PPA-GF40
Denyl HT 5010 PPA-GF50
Denyl HT 5010 Y (PPA+PA66)-GF50
Denyl HT 6010 PPA-GF60
Denyl HT 6010 Y (PPA+PA66)-GF60

Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.