Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of WONDERLOY PC-540A - (PC+ABS) - Chi Mei Corporation

Material Data Center offers the following functions for WONDERLOY PC-540A:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Wonderloy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 20 cm³/10min ISO 1133
Temperatura 260 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 0.5 % ISO 294-4, 2577
ASTM Data
Indice di fluidità a caldo, MFI 20 g/10min ASTM D 1238
Temperatura 260 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 0.005 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Carico unitario a trazione 60 MPa ISO 527
Carico unitario a rottura 55 MPa ISO 527
Modulo a flessione, 23°C 2400 MPa ISO 178
Resistenza alla flessione 90 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 45 kJ/m² ISO 179/1eA
Resistenza all'urto Izod con intaglio, +23°C 45 kJ/m² ISO 180/1A
ASTM Data
Resistenza alla trazione di snervamento 58.9 MPa ASTM D 638
Resistenza alla trazione a rottura 54 MPa ASTM D 638
Allungamento a snervamento 4 % ASTM D 638
Allungamento a rottura 100 % ASTM D 638
Modulo a flessione 2452 MPa ASTM D 790
Resistenza alla flessione 88.3 MPa ASTM D 790
Durezza Rockwell R 119 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 443 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 83 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 108 °C ISO 306
Temp.di rammollimento Vicat, B 101 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 80 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm V-0 class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Reazione al fuoco 5V a spess. h 5VB class IEC 60695-11-20
Spessore provato 2.0 mm -
Yellow Card disponibile - -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 3 mm -
Glow Wire Ignition Temperature (GWIT) 800 °C IEC 60695-2-13
GWIT - thickness tested (1) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 750 °C IEC 60695-2-13
GWIT - thickness tested (2) 3 mm -
ASTM Data
UL 94 combustibilitá V-0 - UL 94
Spessore testati 1.5 mm -
DTUL a 264 psi 86.1 °C ASTM D 648
Temp.di rammollimento Vicat 101 °C ASTM D 1525
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 3.1 - IEC 62631-2-1
Resistività volumica 3.9E15 Ohm*m IEC 62631-3-1
Resistività superficiale 2.9E15 Ohm IEC 62631-3-2
ASTM Data
Rigidità elettrica, breve periodo di tempo 1.26 kV/mm ASTM D 149
Resistenza all’arco 150 s ASTM D 495
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1180 kg/m³ ISO 1183
Densità 1180 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 90 °C -
Pre-essiccamento - Tempo 4 h -
Temperatura dello stampo 50 - 100 °C -
Temperatura - Zona di Alimentazione 200 - 220 °C -
Zona 1 230 - 250 °C -
Temperatura dell ugello 220 - 240 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Additivi
Agente ritardante di fiamma
Caratteristiche speciali
Ritardante di fiamma, Senza alogeni, Stabilizzato o stabile al calore
Applicazioni
IT / Apparecchiature per ufficio, Elettrotecnica ed electrici
Disponibilità geografica
Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.