Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PPcompound G3230A - PP - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PPcompound G3230A:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
SABIC® PPcompound G3230A is a 30% short glass fiber reinforced Polypropylene for under-the-hood and structural applications. The base material is a PP homopolymer and is available in standard black. The glass fibres are chemically coupled to the PP matrix. This material has been designed to combine a good performance profile with fast processing. SABIC® PPcompound G3230A is a designated automotive grade. IMDS ID: 109612410
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 6500 MPa ISO 527
Carico unitario a rottura 93 MPa ISO 527
Deformazione a rottura 3 % ISO 527
Modulo a flessione, 23°C 6900 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 10 kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 11 kJ/m² ISO 179/1eA
ASTM Data
Modulo a trazione 6580 MPa ASTM D 638
Resistenza alla trazione a rottura 83 MPa ASTM D 638
Allungamento a rottura 2.7 % ASTM D 638
Modulo a flessione 5120 MPa ASTM D 790
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 150 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 160 °C ISO 75-1/-2
Temp.di rammollimento Vicat, A 164 °C ISO 306
ASTM Data
DTUL a 66 psi 159 °C ASTM D 648
DTUL a 264 psi 150 °C ASTM D 648
Altre ProprietàValoreUnitáNorma del test
Massa volumica 1130 kg/m³ ISO 1183
Densità 1120 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 80 - 100 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Temperatura di fusione 210 - 270 °C -
Temperatura dello stampo 15 - 60 °C -
Zona 1 190 - 230 °C -
Zona 2 200 - 250 °C -
Zona 3 210 - 270 °C -
Temperatura dell ugello 210 - 270 °C -
Contropressione 1 - 1.5 MPa -
Caratteristiche
Caratteristiche
Omopolimero
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.