Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® PC Resin PC1800R - Europe - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® PC Resin PC1800R - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. It is available exclusively at www.sabicpc.com
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 17 cm³/10min ISO 1133
Temperatura 300 °C -
Carico 1.2 kg -
ASTM Data
Indice di fluidità a caldo, MFI 18 g/10min ASTM D 1238
Temperatura 300 °C -
Carico 1.2 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2350 MPa ISO 527
Carico unitario a trazione 63 MPa ISO 527
Deformazione a snervamento 6 % ISO 527
Deformazione a rottura 50 % ISO 527
Modulo a flessione 2300 MPa ISO 178
Durezza Rockwell R 120 - ISO 2039-2
ASTM Data
Modulo a trazione 2350 MPa ASTM D 638
Resistenza alla trazione di snervamento 63 MPa ASTM D 638
Allungamento a snervamento 6 % ASTM D 638
Allungamento a rottura 70 % ASTM D 638
Modulo a flessione 2300 MPa ASTM D 790
Durezza Rockwell R 120 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 700 J/m ASTM D 256
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 124 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 135 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 141 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm V-2 class IEC 60695-11-10
Spessore provato 1.5 mm -
Conduttività termica 0.2 W/(m K) DIN 52616
ASTM Data
DTUL a 66 psi 135 °C ASTM D 648
DTUL a 264 psi 124 °C ASTM D 648
Temp.di rammollimento Vicat 141 °C ASTM D 1525
Conduttività termica, stato solido 0.0288 W/(m K) ASTM C 177
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 1MHz 3 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 10 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 100 E-4 IEC 62631-2-1
Resistività volumica >1E13 Ohm*m IEC 62631-3-1
Rigidità dielettrica 27 kV/mm IEC 60243-1
ASTM Data
Rigidità elettrica, breve periodo di tempo 27 kV/mm ASTM D 149
Fattore di dissipazione dielèttrica, 60 Hz 0.001 - ASTM D 150
Fattore di dissipazione dielèttrica, 1 MHz 0.01 - ASTM D 150
Costante dielèttrica, 60 Hz 3 - ASTM D 150
Costante dielèttrica, 1 MHz 3 - ASTM D 150
Resistenza di volume 1E15 Ohm*cm ASTM D 257
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 0.8 % ASTM D 1003
Trasmissione luminosa 90 % ASTM D 1003
Indice di rifrazione 1.59 - ASTM D 542
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.35 % Sim. alla ISO 62
Massa volumica 1200 kg/m³ ISO 1183
Assorbimento d’acqua, equilibrio 0.35 % ASTM D 570
Densità 1200 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura ≤120 °C -
Pre-essiccamento - Tempo 2 - 4 h -
Temperatura di fusione 280 - 300 °C -
Temperatura dello stampo 80 - 100 °C -
Zona 1 260 - 280 °C -
Zona 2 270 - 290 °C -
Zona 3 280 - 300 °C -
Temperatura dell ugello 270 - 290 °C -
Caratteristiche
Caratteristiche speciali
Stabilizzato o stabile al calore
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.