Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SABIC® LLDPE 118WE - (PE-LLD) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for SABIC® LLDPE 118WE:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Sabic datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
SABIC® LLDPE 118WE is a butene-linear low density polyethylene resin for general purpose applications. Films produced from this resin are tough with excellent puncture resistance, high tensile strength, good hottack properties and low gel levels. The resin contains anti block and slip agent. Application Typical applications for SABIC® LLDPE 118WE are shipping sacks, ice bags, frozen food bags, liners, carrier bags, garbage bags, agriculture films, lamination and coextruded films, shrink film (for blending with LDPE), industrial consumer packaging and high clarity film if blended with (10-20%) LDPE. Film properties Film of 50 ?m and BUR=2 has been produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 2,7 mm. The product mentioned
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di rammollimento Vicat, A 101 °C ISO 306
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 20 % ASTM D 1003
Proprietà Meccaniche (Film)ValoreUnitáNorma del test
ISO Data
Modulo a trazione, parallelo 160 MPa ISO 527-3
Modulo a trazione, perpend. 180 MPa ISO 527-3
Carico allo snervamento, normal 11 MPa ISO 527-3
Carico unitario a rottura, parallelo 37 MPa ISO 527-3
Carico unitario a rottura, perpend. 30 MPa ISO 527-3
Resistenza alla lacerazione Trouser, parallel 40 N/mm ISO 6383-1
Resistenza alla lacerazione Trouser, normal 120 N/mm ISO 6383-1
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.