Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin PX9406P - Americas - (PPE+PS) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin PX9406P - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
NORYL™ PX9406P resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of 5VA at 2.5mm and V0 at 0.75mm. NORYL PX9406P is VDE certified IEC60335 and offers strong electrical performance at thin wall, high heat resistance, Low Warpage, low moisture absorption, and dimensional stability. This material is an excellent candidate for unattended appliance applications such as printed circuit board (PCB) holders, terminal blocks + connectors, circuit protection / relay / switches, motor end caps, control box / panels, and battery charger / fuse holders where VDE IEC60335 is required.

UL Yellow Card Link E121562-101325735
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 10 cm³/10min ISO 1133
Temperatura 280 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 2600 MPa ISO 527
Carico unitario a trazione 73 MPa ISO 527
Deformazione a snervamento 4.5 % ISO 527
Carico unitario a rottura 55 MPa ISO 527
Deformazione a rottura 8 % ISO 527
Modulo a flessione 2500 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 11 kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 8 kJ/m² ISO 179/1eA
Resist. urto Izod con intaglio, +23°C, 4mm 10 kJ/m² ISO 180/1A
Resist. urto Izod con intaglio, -30°C, 4mm 6 kJ/m² ISO 180/1A
ASTM Data
Modulo a trazione 2800 MPa ASTM D 638
Resistenza alla trazione di snervamento 76 MPa ASTM D 638
Resistenza alla trazione a rottura 55 MPa ASTM D 638
Allungamento a snervamento 4.7 % ASTM D 638
Allungamento a rottura 9.7 % ASTM D 638
Modulo a flessione 2840 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 140 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 60 J/m ASTM D 256
Temperatura -30 °C -
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 117 °C ISO 75-1/-2
Temp.di rammollimento Vicat, 120°C/h 10N 150 °C ISO 306
Temp.di rammollimento Vicat, 120°C/h 50N 140 °C ISO 306
Reazione al fuoco a spessore h V-2 class IEC 60695-11-10
Spessore provato 0.4 mm -
Reazione al fuoco 5V a spess. h 5VB class IEC 60695-11-20
Spessore provato 2.0 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 775 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
DTUL a 264 psi 118 °C ASTM D 648
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Res. Alle correnti striscianti superficiali 250 - IEC 60112
Altre ProprietàValoreUnitáNorma del test
Densità 1100 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 105 - 110 °C -
Pre-essiccamento - Tempo 3 - 4 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 275 - 305 °C -
Temperatura dello stampo 70 - 100 °C -
Zona 1 245 - 295 °C -
Zona 2 255 - 300 °C -
Zona 3 265 - 305 °C -
Velocità di Rotazione della Vite 20 - 100 rpm -
Contropressione 0.3 - 0.7 MPa -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Additivi
Agente ritardante di fiamma
Caratteristiche speciali
Ritardante di fiamma
Disponibilità geografica
Nord America
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.