Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL™ Resin GFN1F - Asia - (PPE+PS)-GF10 - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL™ Resin GFN1F - Asia:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
NORYL™ GFN1F resin is a 10% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN1F carries a UL746C outdoor suitability rating of F1 along with FDA food contact compliance and NSF 61 listings in several colors. The properties of this material makes it an excellent candidate for water management applications such as water filter and meter components, pump housings / impellers, shower + faucet, and valves.*See NORYL GFN1 resin for NON FDA / NSF version.

UL Yellow Card Link E45587-237019
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 4 cm³/10min ISO 1133
Temperatura 280 °C -
Carico 5 kg -
ASTM Data
Indice di fluidità a caldo, MFI 4 g/10min ASTM D 1238
Temperatura 280 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3900 MPa ISO 527
Carico unitario a trazione 60 MPa ISO 527
Deformazione a snervamento 4.5 % ISO 527
Carico unitario a rottura 60 MPa ISO 527
Deformazione a rottura 4.5 % ISO 527
Modulo a flessione 3700 MPa ISO 178
Resist. urto Charpy con intaglio, +23°C 8 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm 30 kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm 30 kJ/m² ISO 180/1U
Resist. urto Izod con intaglio, +23°C, 4mm 10 kJ/m² ISO 180/1A
Resist. urto Izod con intaglio, -30°C, 4mm 9 kJ/m² ISO 180/1A
ASTM Data
Modulo a trazione 4400 MPa ASTM D 638
Resistenza alla trazione di snervamento 75 MPa ASTM D 638
Resistenza alla trazione a rottura 75 MPa ASTM D 638
Allungamento a snervamento 3.5 % ASTM D 638
Allungamento a rottura 3.5 % ASTM D 638
Modulo a flessione 3400 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 84 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 80 J/m ASTM D 256
Temperatura -30 °C -
Resistenza all'urto Izod, 1/8 in 410 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di inflessione sotto carico, 1.80 MPa 129 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 138 °C ISO 306
Temp.di rammollimento Vicat, 120°C/h 50N 140 °C ISO 306
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
ASTM Data
DTUL a 66 psi 135 °C ASTM D 648
DTUL a 264 psi 130 °C ASTM D 648
Temp.di rammollimento Vicat 138 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.12 % Sim. alla ISO 62
Assorbimento d'umidità 0.04 % Sim. alla ISO 62
Massa volumica 1170 kg/m³ ISO 1183
Densità 1170 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 105 - 110 °C -
Pre-essiccamento - Tempo 3 - 4 h -
Umidità del Processo ≤0.02 % -
Temperatura di fusione 295 - 315 °C -
Temperatura dello stampo 75 - 105 °C -
Zona 1 260 - 305 °C -
Zona 2 270 - 310 °C -
Zona 3 280 - 315 °C -
Velocità di Rotazione della Vite 20 - 100 rpm -
Contropressione 0.3 - 0.7 MPa -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Resistenza Chimica
Stabilità idrolitica
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Disponibilità geografica
Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.