Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grivory HT2VZ-15H black 9205 - PA6T/66-GF15 - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grivory HT2VZ-15H black 9205:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Grivory datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Product-nomenclature: ISO 16396-PA6T/66,GF15,M1H,C12-060

 

Co Polyamide

Partially aromatic Polyamide

Product Attributes

  Improved alcohol resistance, Improved impact resistance, Improved heat resistance

Markets

  Automotive
  Air intake sytems, Compressed air systems, Hydraulic systems,
Automotive electr. and electronics, lighting, Fuel systems, Powertrain and Chassis, Interior
  Electricals & Electronics
  Electrical appliances, Electrical equipment, Connectors, Energy distribution,
Mobile phones and other portable devices
  Industry & Consumer goods
  Hydraulics & Pneumatics, Mechanical Engineering, Power transmission, Tools & Accessories
Caratteristiche Fisichesecco/condUnitáNorma del test
ISO Data
Ritiro di stampaggio, parallelo 0.4 / * % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 0.9 / * % ISO 294-4, 2577
Proprietà Meccanichesecco/condUnitáNorma del test
ISO Data
Modulo a trazione 6000 / 5800 MPa ISO 527
Carico unitario a rottura 125 / 100 MPa ISO 527
Deformazione a rottura 3 / 3.5 % ISO 527
Resistenza all'urto Charpy, +23°C 65 / 55 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 45 / 40 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 10 / 10 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 5 / 5 kJ/m² ISO 179/1eA
Durezza Shore D 82 / * - ISO 7619-1
Proprietà Termichesecco/condUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 310 / * °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 265 / * °C ISO 75-1/-2
Temp.di inflessione sotto caricor, 8.00 MPa 100 / * °C ISO 75-1/-2
Coeff.di dilatazione termica lin., parallelo 30 / * E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 75 / * E-6/K ISO 11359-1/-2
Reazione al fuoco a spessore h HB / * class IEC 60695-11-10
Spessore provato 0.8 / * mm -
Proprietà Elettrichesecco/condUnitáNorma del test
ISO Data
Resistività volumica 1E10 / 1E10 Ohm*m IEC 62631-3-1
Resistività superficiale * / 1E12 Ohm IEC 62631-3-2
Rigidità dielettrica 33 / 32 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali - / 575 - IEC 60112
Altre Proprietàsecco/condUnitáNorma del test
Assorbimento d'acqua 5.5 / * % Sim. alla ISO 62
Assorbimento d'umidità 2 / * % Sim. alla ISO 62
Massa volumica 1240 / - kg/m³ ISO 1183
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione
Forma fisica disponibile
Granuli, Nero
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore
Caratteristiche
Copolimero
Applicazioni
Automotive, Elettrotecnica ed electrici
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.