Caratteristiche Fisiche | Valore | Unitá | Norma del test |
Other Standards[S] |
Ritiro di stampaggio, parallelo |
0.002 |
mm/mm |
|
Ritiro di stampaggio, perpend. |
0.005 |
mm/mm |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Meccaniche | Valore | Unitá | Norma del test |
Other Standards[S] |
Resistenza alla trazione |
150 |
MPa |
|
Resistenza a compressione |
110 |
MPa |
|
Modulo a flessione |
17000 |
MPa |
|
Resistenza alla flessione |
220 |
MPa |
|
Durezza Rockwell |
R 110 |
- |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Termiche | Valore | Unitá | Norma del test |
ASTM Data |
UL 94 combustibilitá |
V-0 |
- |
UL 94 |
Spessore testati |
2 |
mm |
- |
Other Standards[S] |
coefficiente d’espansione termica, lung. |
18 |
E-6/K |
|
DTUL a 264 psi |
267 |
°C |
|
Temperatura di fusione |
288 |
°C |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Proprietà Elettriche | Valore | Unitá | Norma del test |
Other Standards[S] |
Rigidità elettrica, breve periodo di tempo |
15 |
kV/mm |
|
Costante dielèttrica, 1 MHz |
5 |
- |
|
Resistenza superficiale |
>1E15 |
Ohm |
|
Resistenza di volume |
>1E15 |
Ohm*cm |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Altre Proprietà | Valore | Unitá | Norma del test |
Other Standards[S] |
Densità |
1800 |
kg/m³ |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Caratteristiche
Disponibilità geografica
Asia Oceano Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com