Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 500P NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 500P NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.


Delrin® 500P is a general purpose medium viscosity acetal homopolymer for injection molding.  It has improved processing thermal stability, a good combination of mechanical properties, and low VOC emissions.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 13 cm³/10min ISO 1133
Temperatura 190 °C -
Carico 2.16 kg -
Ritiro di stampaggio, parallelo 2.0 % ISO 294-4, 2577
Ritiro di stampaggio, perpendicolare 1.9 % ISO 294-4, 2577
ASTM Data
Indice di fluidità a caldo, MFI 7 g/10min ASTM D 1238
Temperatura 190 °C -
Carico 1.05 kg -
Ritiro di stampaggio, parallelo 0.0195 mm/mm ASTM D 955
Ritiro di stampaggio, perpend. 0.0195 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 3100 MPa ISO 527
Carico unitario a trazione 71 MPa ISO 527
Deformazione a snervamento 17 % ISO 527
Deformazione nominale a rottura 30 % ISO 527
Modulo di scorrimento a trazione, 1h 2800 MPa ISO 899-1
Modulo di scorrimento a trazione, 1000h 1600 MPa ISO 899-1
Resistenza all'urto Charpy, +23°C 300 kJ/m² ISO 179/1eU
Resistenza all'urto Charpy, -30°C 280 kJ/m² ISO 179/1eU
Resistenzia all'urto Charpy con intaglio, +23°C 9 kJ/m² ISO 179/1eA
Resistenzia all'urto Charpy con intaglio, -30°C 8 kJ/m² ISO 179/1eA
Perforazione-forza massima, +23°C 2000 N ISO 6603-2
Energia di perforazione, +23°C 3 J ISO 6603-2
ASTM Data
Modulo a trazione 3250 MPa ASTM D 638
Resistenza alla trazione 68 MPa ASTM D 638
Resistenza alla trazione di snervamento 68 MPa ASTM D 638
Allungamento a snervamento 15 % ASTM D 638
Allungamento a rottura 40 % ASTM D 638
Modulo a flessione 3100 MPa ASTM D 790
Durezza Rockwell R 120 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 75 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 178 °C ISO 11357-1/-3
Temp.di inflessione sotto carico, 1.80 MPa 93 °C ISO 75-1/-2
Temp.di inflessione sotto carico, 0.45 MPa 160 °C ISO 75-1/-2
Temp.di rammollimento Vicat, B 155 °C ISO 306
Coeff.di dilatazione termica lin., parallelo 100 E-6/K ISO 11359-1/-2
Coeff.di dilatazione termica lin., perpend. 100 E-6/K ISO 11359-1/-2
Reaz. al fuoco spess.nom. 1.5mm HB class IEC 60695-11-10
Spessore provato 1.5 mm -
Yellow Card disponibile - -
Reazione al fuoco a spessore h HB class IEC 60695-11-10
Spessore provato 0.8 mm -
Yellow Card disponibile - -
Indice di ossigeno 22 % ISO 4589-1/-2
ASTM Data
UL 94 combustibilitá HB - UL 94
Spessore testati 1.5 mm -
coefficiente d’espansione termica, lung. 113 E-6/K ASTM D 696
Coefficiente d’espansione termica, tras. 109 E-6/K ASTM D 696
DTUL a 66 psi 167 °C ASTM D 648
DTUL a 264 psi 102 °C ASTM D 648
Temperatura di fusione 178 °C ASTM D 3418
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Costante dielettrica relativa, 100Hz 3.8 - IEC 62631-2-1
Costante dielettrica relativa, 1MHz 3.8 - IEC 62631-2-1
Fattore di dissipazione, 100Hz 90 E-4 IEC 62631-2-1
Fattore di dissipazione, 1MHz 90 E-4 IEC 62631-2-1
Resistività volumica 2E12 Ohm*m IEC 62631-3-1
Resistività superficiale 4E14 Ohm IEC 62631-3-2
Rigidità dielettrica 44 kV/mm IEC 60243-1
Res. Alle correnti striscianti superficiali 600 - IEC 60112
ASTM Data
Rigidità elettrica, breve periodo di tempo 17.3 kV/mm ASTM D 149
Fattore di dissipazione dielèttrica, 1 MHz 0.005 - ASTM D 150
Costante dielèttrica, 1 MHz 3.7 - ASTM D 150
Resistenza superficiale 2E14 Ohm ASTM D 257
Resistenza di volume 1E14 Ohm*cm ASTM D 257
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 1.3 % Sim. alla ISO 62
Assorbimento d'umidità 0.2 % Sim. alla ISO 62
Massa volumica 1420 kg/m³ ISO 1183
Assorbimento d’acqua, 24hr 0.4 % ASTM D 570
Assorbimento d’acqua, equilibrio 0.28 % ASTM D 570
Densità 1420 kg/m³ ASTM D 792
Funzioni
Viscosità-Velocità di taglio , Delrin® 500P NC010, POM, DuPont
Sforzo di taglio-Velocità di taglio , Delrin® 500P NC010, POM, DuPont
Modulo dinamico a taglio-temperatura , Delrin® 500P NC010, POM, DuPont
Sforzi-deformazione , Delrin® 500P NC010, POM, DuPont
Modulo secante-deformazione , Delrin® 500P NC010, POM, DuPont
Sforzi-deformazioni (isocrona) 23°C, Delrin® 500P NC010, POM, DuPont
Modulo di scorrimento-tempo 23°C, Delrin® 500P NC010, POM, DuPont
Curva di scorrimento 23°C, Delrin® 500P NC010, POM, DuPont
Volume specifico-temperatura (pvT) , Delrin® 500P NC010, POM, DuPont
Modulo a taglio-temperatura , Delrin® 500P NC010, POM, DuPont
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Estrusione Film, Estrusione di tubi, Estrusione Profilati, Estrusione di Lastre/Fogli, Estrusione cavi, Altre Estrusioni
Forma fisica disponibile
Pellet, Colore naturale
Additivi
Lubrificanti, Agente di distacco
Caratteristiche speciali
Alto urto o modificato all'urto
Caratteristiche
Resistenza al scorrimento, Resistenza alla fatica, Low Emission, Stabilità termica, Saldabile, Omopolimero
Applicazioni
Polivalente
Disponibilità geografica
Altre informazioni
Stampaggio ad Iniezione
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

Resistenza chimica
Acidi
Acido acetico (5% da massa) (23°C)
Soluzione acida citrica (10% da massa) (23°C)
Acido lattico (10% da massa) (23°C)
Acido cloridrico (36% da massa) (23°C)
Acido nitrico (40% da massa) (23°C)
Acido solforico (38% da massa) (23°C)
Acido solforico (5% da massa) (23°C)
Soluzione acida cromica (40% da massa) (23°C)
Basi
Soluzione dell' idrossido del sodio (35% da massa) (23°C)
Soluzione dell' idrossido del sodio (1% da massa) (23°C)
Soluzione dell' idrossido di ammonio (10% da massa) (23°C)
Alcool
Alcool di isopropile (23°C)
Metanolo (23°C)
Etanolo (23°C)
Idrocarburi
n-Hexane (23°C)
Toluene (23°C)
isoottano (23°C)
Chetoni
Acetone (23°C)
Eteri
Etere Etilico (23°C)
Oli minerali
Olio multigrade del motore di SAE 10W40 (23°C)
Olio multigrade del motore di SAE 10W40 (130°C)
Olio dell' ipoide-ingranaggio di SAE 80/90 (130°C)
Olio isolante (23°C)
Combustibili Standard
Liquido 1 di ISO 1817 (60°C)
Liquido 2 di ISO 1817 (60°C)
Liquido 3 di ISO 1817 (60°C)
Liquido 4 di ISO 1817 (60°C)
Combust. stand. senza alcool (pref. ISO 1817 liquido C) (23°C)
Combust. stand. con alcool (pref. ISO 1817 liquido 4) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (23°C)
Combustibile diesel (pref. ISO 1817 liquido F) (90°C)
Combustibile diesel (pref. ISO 1817 liquido F) (>90°C)
Diesel EN 590 (100°C)
Soluzioni saline
Soluzione del cloruro di sodio (10% da massa) (23°C)
Soluzione dell' ipoclorito del sodio (10% da massa) (23°C)
Soluzione del carbonato di sodio (20% da massa) (23°C)
Soluzione del carbonato di sodio (2% da massa) (23°C)
Soluzione del cloruro dello zinco (50% da massa) (23°C)
Altri
Acetato etilico (23°C)
Perossido di idrogeno (23°C)
Liquido di freno del DOT N° 4 (130°C)
Glicol etilenico (50% da massa) in acqua (108°C)
etanolo di nonylphenoxy-polyethyleneoxy 1% in acqua (23°C)
acido oleico 50% + olio di oliva 50% (23°C)
Acqua (23°C)
Acqua deionizzata (90°C)
Soluzione del fenolo (5% da massa) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.