Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Tritan™ EX401 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Tritan™ EX401:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Tritan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto

Tritan EX401, specifically developed for the Infant Care market, is an amorphous copolyester with excellent appearance and clarity. Tritan EX401 contains a mold release derived from vegetable based sources. Its most outstanding features are clarity, excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan EX401 meets infant care sterilization requirements via boiling water or microwave steam sterilization. This newgeneration copolyester can also be molded into various applications without incorporating high levels of residual stress. Combined with Tritan's outstanding chemical resistance and hydrolytic stability, these features give molded products enhanced durability in the dishwasher environment, which can expose products to high heat, humidity, and aggressive cleaning agents.

Tritan EX401 can be converted into parts using injection molding, injection stretch blow molding (ISBM), and extrusion blow molding techniques.

Tritan EX401 may be used in repeated use food contact articles under United States Food and Drug Administration (FDA) regulations. Contact Eastman representative for details on global food contact regulatory clearances.




Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Ritiro di stampaggio, parallelo 0.006 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 1620 MPa ISO 527
Carico unitario a trazione 45 MPa ISO 527
Deformazione a snervamento 7 % ISO 527
Carico unitario a rottura 49 MPa ISO 527
Deformazione a rottura 130 % ISO 527
Modulo a flessione, 23°C 1530 MPa ISO 178
Resistenza all'urto Izod con intaglio, +23°C 66 kJ/m² ISO 180/1A
Resistenza all'urto Izod con intaglio 14 kJ/m² ISO 180/1A
Temperatura -40 °C -
ASTM Data
Modulo a trazione 1585 MPa ASTM D 638
Resistenza alla trazione di snervamento 44 MPa ASTM D 638
Resistenza alla trazione a rottura 53.1 MPa ASTM D 638
Allungamento a snervamento 7 % ASTM D 638
Allungamento a rottura 140 % ASTM D 638
Modulo a flessione 1585 MPa ASTM D 790
Durezza Rockwell R 115 - ASTM D 785
Resistenza all'urto Izod con intaglio, 1/8 in 650 J/m ASTM D 256
Resistenza all'urto Izod con intaglio, basso temperatura 126 J/m ASTM D 256
Temperatura -40 °C -
Resistenza all'urto Izod, 1/8 in N J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 109 °C ASTM D 648
DTUL a 264 psi 92 °C ASTM D 648
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 1 % ASTM D 1003
Trasmissione luminosa 92 % ASTM D 1003
Altre ProprietàValoreUnitáNorma del test
Densità 1170 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 88 °C -
Pre-essiccamento - Tempo 4 - 6 h -
Temperatura di fusione 260 - 282 °C -
Temperatura dello stampo 38 - 66 °C -
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Pre-essiccamento - Temperatura 88 °C -
Pre-essiccamento - Tempo 4 - 6 h -
Temperatura di fusione 240 - 250 °C -
Temperatura dello stampo 25 - 45 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Soffiaggio
Additivi
Agente di distacco
Caratteristiche speciali
Alto urto o modificato all'urto, Stabilizzato o stabile al calore, Trasparente, Sterilizzabile, Sterilizzazione a vapore
Caratteristiche
Amorfo, Copolimero
Resistenza Chimica
Resistenza chimica generale, Stabilità idrolitica
Certifications
Contatto con gli alimenti, Approvato per l'utilizzo per contatto con alimenti secondo la FDA 21 CFR
Disponibilità geografica
Nord America, Europa, Asia Oceano Pacifico, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.