Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styroflex® 4G80 - SB - INEOS Styrolution

Material Data Center offers the following functions for Styroflex® 4G80:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Styroflex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 18 cm³/10min ISO 1133
Temperatura 200 °C -
Carico 5 kg -
ASTM Data
Indice di fluidità a caldo, MFI 76 g/10min ASTM D 1238
Temperatura 220 °C -
Carico 10 kg -
Ritiro di stampaggio, parallelo 0.006 mm/mm ASTM D 955
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 50 MPa ISO 527
Deformazione a rottura 500 % ISO 527
Resist. urto Charpy con intaglio, +23°C 80 kJ/m² ISO 179/1eA
Resist. urto Charpy con intaglio, -30°C 80 kJ/m² ISO 179/1eA
Durezza Shore A 80 - ISO 7619-1
Durezza Shore D 28 - ISO 7619-1
ASTM Data
Modulo a trazione 68.95 MPa ASTM D 638
Resistenza alla trazione di snervamento 2.41 MPa ASTM D 638
Allungamento a rottura 500 % ASTM D 638
Durezza A Shore 80 - ASTM D 2240
Durezza D Shore 28 - ASTM D 2240
Resistenza all'urto Izod con intaglio, 1/8 in 747 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temp.di rammollimento Vicat, A 38 °C ISO 306
ASTM Data
Temp.di rammollimento Vicat 39.4 °C ASTM D 1525
Proprietà OtticheValoreUnitáNorma del test
ASTM Data
Opacità 18 % ASTM D 1003
Trasmissione luminosa 81 % ASTM D 1003
Indice di rifrazione 1.56 - ASTM D 542
Altre ProprietàValoreUnitáNorma del test
Assorbimento d'acqua 0.07 % Sim. alla ISO 62
Assorbimento d'umidità 0.07 % Sim. alla ISO 62
Massa volumica 980 kg/m³ ISO 1183
Densità 980 kg/m³ ASTM D 792
Raccomandazione de Processabilità EstrusioneValoreUnitáNorma del test
Temperatura di fusione 170 - 240 °C -
Temperatura dello stampo 29.4 - 43.3 °C -
Caratteristiche
Processabilità e Forma di Forni
Altre Estrusioni
Forma fisica disponibile
Pellet
Caratteristiche speciali
Trasparente
Caratteristiche
Soft Feel, Copolimero
Applicazioni
Medicale, Attrezzature sportive
Disponibilità geografica
Nord America, Europa, South and Central America, Near East/Africa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.