Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Halene - P M212S - PP - Haldia Petrochemicals

Material Data Center offers the following functions for Halene - P M212S:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Halene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caratteristiche FisicheValoreUnitáNorma del test
ASTM Data
Indice di fluidità a caldo, MFI 12 g/10min ASTM D 1238
Temperatura 230 °C -
Carico 2.16 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ASTM Data
Resistenza alla trazione di snervamento 28 MPa ASTM D 638
Allungamento a snervamento 12 % ASTM D 638
Modulo a flessione 1050 MPa ASTM D 790
Resistenza all'urto Izod con intaglio, 1/8 in 50 J/m ASTM D 256
Proprietà TermicheValoreUnitáNorma del test
ASTM Data
DTUL a 66 psi 75 °C ASTM D 648
Temp.di rammollimento Vicat 128 °C ASTM D 1525
Altre ProprietàValoreUnitáNorma del test
Densità 900 kg/m³ ASTM D 792
Raccomandazione de Processabilità Stampaggio ad IniezioneValoreUnitáNorma del test
Temperatura dello stampo 30 - 60 °C -
Zona 1 160 - 250 °C -
Caratteristiche
Processabilità e Forma di Forni
Stampaggio ad Iniezione, Soffiaggio
Caratteristiche speciali
Trasparente
Caratteristiche
High Gloss, Copolimero, Copolimero casuale
Disponibilità geografica
Asia Oceano Pacifico
Altre informazioni
Stampaggio ad Iniezione
M212S is a Clarified Polypropylene Random Copolymer produced by Spheripol Technology.

M212S combines excellent Clarity, Gloss, High Flow, Low Cycle Time and Stiffness – Impact balance.

M212S is recommended for high clarity Injection Molded & Injection Stretch Blow Molded (ISBM) Containers, Household items, Injection Syringes.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.