Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® MB 3000 NAT - PA11... - ARKEMA

Material Data Center offers the following functions for Rilsan® MB 3000 NAT:
unit conversion, PDF datasheet print, comparison with other plastics, parameters for material models, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
PA11, MHLF, 12-020, MD
Rilsan® MB 3000 NAT resin is a polyamide 11 produced from a renewable source. This natural grade is designed for injection molding and is classified as Halogen Free Flame Retardant (HFFR).

The percentage of renewable carbon according to ASTM D 6866 (calculated) is >90%.


Main applications:
  • Wire and cable sheathing
  • Elevator doors rollers

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 95 / * cm³/10min ISO 1133
Température 235 / * °C -
Charge 2.16 / * kg -
Retrait au moulage, parallèle 0.9 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.9 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction - / 1830 MPa ISO 527
Contrainte d'écoulement 45 / 45 MPa ISO 527
Déformation au seuil d'écoulement 5 / 5 % ISO 527
Déformation nominale à la rupture >50 / >50 % ISO 527
Résistance au choc Charpy, +23°C - / 83 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C - / 38 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C - / 4 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C - / 3 kJ/m² ISO 179/1eA
Dureté Shore D 69 / * - ISO 7619-1
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 189 / * °C ISO 11357-1/-3
Coeffic. de dilatation therm. linéique, parallèle 102 / * E-6/K ISO 11359-1/-2
Inflammabilité ep. nom. 1.5 mm V-0 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 1.6 / * mm -
Yellow Card disponible oui / * - -
Inflammabilité pr. épaisseur h V-0 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Yellow Card disponible oui / * - -
Aptitude à l'allumage 33 / * % ISO 4589-1/-2
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3 / - - IEC 62631-2-1
Permittivité relative, 1MHz 3 / - - IEC 62631-2-1
Facteur de pertes, 100Hz 221 / - E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 180 / - E-4 IEC 62631-2-1
Résistivité transversale >1E13 / >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle * / >1E15 Ohm IEC 62631-3-2
Rigidité diélectrique 28 / 28 kV/mm IEC 60243-1
Indice de résistance au cheminement * / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 2 / * % Sim. to ISO 62
Absorption d'humidité 0.6 / * % Sim. to ISO 62
Masse volumique 1090 / 1090 kg/m³ ISO 1183
Biobased content 90 % -
Fonctions
Viscosité / Vitesse de cisaillement , Rilsan® MB 3000 NAT, PA11..., ARKEMA
Contrainte de cisaillement / Vit. de cisaillement , Rilsan® MB 3000 NAT, PA11..., ARKEMA
Module de cisaillement dynamique / Température , Rilsan® MB 3000 NAT (sec), PA11..., ARKEMA
Contrainte / Déformation , Rilsan® MB 3000 NAT (sec), PA11..., ARKEMA
Module sécant / Déformation , Rilsan® MB 3000 NAT (sec), PA11..., ARKEMA
Caractéristiques
Transformation
Moulage par injection
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant
Propriétés spéciales
Ignifugé, Stabilisé à la lumière, Stabilisé aux intempéries, Stabilisé à la chaleur
Certifications
Contient des ressources renouvelables
Disponibilité régionale
Autres informations
Moulages par injection

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 220°C / 230°C.
- Mold temperature : 20 - 60°C

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80-90°C.

Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.