Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUMIPLAS LD590T - ABS - LG Chem

Material Data Center offers the following functions for LUMIPLAS LD590T:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Lumiplas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ASTM Data
Indice de fluidité, MFI 8 g/10min ASTM D 1238
Température 220 °C -
Charge 10 kg -
Retrait au moulage , parallèle 0.0055 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ASTM Data
Résistance de traction à la rupture 49 MPa ASTM D 638
Allongement à la rupture 30 % ASTM D 638
Module de flexion 2453 MPa ASTM D 790
Résistance à la flexion 78.5 MPa ASTM D 790
Dureté Rockwell R 108 - ASTM D 785
Izod choc avec entaille, 1/8 in 104 J/m ASTM D 256
Izod choc avec entaille, 1/4 in 94.3 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ASTM Data
coefficient de dilatation thermique, long. 84 E-6/K ASTM D 696
DTUL à 264 psi 81 °C ASTM D 648
Propriétés diversesValeurUnitéNorme du test
Densité 1120 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 70 - 80 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.01 % -
Température de la matière fondue 230 - 250 °C -
Température du moule 40 - 60 °C -
Zone 1 190 - 210 °C -
Zone 2 200 - 220 °C -
Zone 3 220 - 250 °C -
Température de la buse 230 - 250 °C -
Vitesse de rotation de vis 30 - 60 rpm -
Contre-pression 1 - 4 MPa -
Recommandations pour la transformation ExtrusionValeurUnitéNorme du test
Pré-séchage - température 70 - 80 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.01 % -
Température de la matière fondue 230 - 250 °C -
Zone 1 190 - 210 °C -
Zone 2 200 - 230 °C -
Zone 3 210 - 240 °C -
Zone 4 220 - 250 °C -
Température de la buse 220 - 250 °C -
Caractéristiques
Transformation
Moulage par injection, Extrusion (autres)
Propriétés spéciales
Modifié choc
Caractéristiques
Light Diffusing
Applications
Électrotechnique et électrique
Disponibilité régionale
Amérique du nord, Europe, Asia Pacific, South and Central America
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.