Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LEXAN™ VISUALFX™ Resin LUX7630C - Americas - PC - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for LEXAN™ VISUALFX™ Resin LUX7630C - Americas:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lexan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
LEXAN LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is UV stabilized (F1 rating) providing additional weathering capability. LEXAN LUX7630C is available in transparent natural colors only.

UL Yellow Card Link E121562-101088456
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 5 cm³/10min ISO 1133
Température 300 °C -
Charge 1.2 kg -
ASTM Data
Indice de fluidité, MFI 5 g/10min ASTM D 1238
Température 300 °C -
Charge 1.2 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2400 MPa ISO 527
Contrainte d'écoulement 67 MPa ISO 527
Déformation au seuil d'écoulement 6 % ISO 527
Contrainte à la rupture 52 MPa ISO 527
Déformation à la rupture 23 % ISO 527
Module de flexion 2500 MPa ISO 178
Résistance au choc Charpy, +23°C, 3mm N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C, 3mm N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C, 3mm 10 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C, 3mm 9 kJ/m² ISO 179/1eA
Résistance au choc Izod, +23°C N kJ/m² ISO 180/1U
Résistance au choc Izod (entaillé), +23°C, 3mm 10 kJ/m² ISO 180/1A
Résistance au choc Izod (entaillé), -30°C, 3mm 9 kJ/m² ISO 180/1A
ASTM Data
Module en traction 2500 MPa ASTM D 638
Module de traction d’élasticité 68 MPa ASTM D 638
Résistance de traction à la rupture 52 MPa ASTM D 638
Allongement d’élasticité 6 % ASTM D 638
Allongement à la rupture 51 % ASTM D 638
Module de flexion 2400 MPa ASTM D 790
Izod choc avec entaille, 1/8 in 100 J/m ASTM D 256
Izod choc avec entaille, bas température 85 J/m ASTM D 256
Température -30 °C -
Résistance au choc Izod, 1/8 in N J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, B 137 °C ISO 306
Température de ramolliss. Vicat, 120°C/h 50N 139 °C ISO 306
Inflammabilité pr. épaisseur h V-2 class IEC 60695-11-10
Epaisseur de l'éprouvette 0.4 mm -
Inflammabilité 5V pr. épaisseur h 5VA class IEC 60695-11-20
Epaisseur de l'éprouvette 3.0 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
ASTM Data
DTUL à 66 psi 131 °C ASTM D 648
DTUL à 264 psi 120 °C ASTM D 648
Vicat température 136 °C ASTM D 1525
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Rigidité diélectrique 36.2 kV/mm IEC 60243-1
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 0.14 % Sim. to ISO 62
Absorption d'humidité 0.11 % Sim. to ISO 62
Masse volumique 1200 kg/m³ ISO 1183
Densité 1190 kg/m³ ASTM D 792
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 120 °C -
Pré-séchage - temps 3 - 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 290 - 310 °C -
Température du moule 70 - 95 °C -
Zone 1 265 - 290 °C -
Zone 2 275 - 300 °C -
Zone 3 290 - 310 °C -
Vitesse de rotation de vis 40 - 70 rpm -
Contre-pression 0.3 - 0.7 MPa -
Caractéristiques
Transformation
Moulage par injection
Additifs
Agent ignifugeant
Propriétés spéciales
Ignifugé, Transparent
Disponibilité régionale
Amérique du nord
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.