Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Grilamid TR 30 natural - PA* - EMS-GRIVORY | a unit of EMS-CHEMIE AG

Material Data Center offers the following functions for Grilamid TR 30 natural:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Grilamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Product-nomenclature: ISO 16396-PA 6I/X,,GT,C12-030

 

Co Polyamide

Partially aromatic Polyamide

Transparent Polyamide

Product Attributes

  Hydrolysis resistant, Highly transparent, Barrier material

Markets

  Automotive
  Compressed air systems, Automotive electr. and electronics, lighting, Cooling and climate control,
Fuel systems, Powertrain and Chassis, Interior
  Electricals & Electronics
  Electrical appliances, Electrical equipment, Connectors, Energy distribution,
Mobile phones and other portable devices, Lighting
  Industry & Consumer goods
  Medical devices
  Packaging
  Injectionstretchblowmoulded containers

Approvals

  Burning Behaviour
  UL V2
  Food Contact
  EU Requirements, FDA
Caractéristiques des transformations/physiquessec / condUnitéNorme du test
ISO Data
Retrait au moulage, parallèle 0.7 / * % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 0.7 / * % ISO 294-4, 2577
Propriétés mécaniquessec / condUnitéNorme du test
ISO Data
Module en traction - / 2800 MPa ISO 527
Contrainte d'écoulement - / 90 MPa ISO 527
Déformation au seuil d'écoulement - / 6 % ISO 527
Déformation nominale à la rupture - / >50 % ISO 527
Résistance au choc Charpy, +23°C - / N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C - / N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C - / 12 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C - / 12 kJ/m² ISO 179/1eA
Propriétés thermiquessec / condUnitéNorme du test
ISO Data
Température de transition vitreuse, 10°C/min 160 / * °C ISO 11357-1/-2
Température de fléchissement s/chrg, 1.80 MPa 125 / * °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 135 / * °C ISO 75-1/-2
Coeffic. de dilatation therm. linéique, parallèle 60 / * E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 60 / * E-6/K ISO 11359-1/-2
Inflammabilité pr. épaisseur h V-2 / * class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 / * mm -
Propriétés électriquessec / condUnitéNorme du test
ISO Data
Résistivité transversale - / 1E11 Ohm*m IEC 62631-3-1
Résistivité superficielle * / 1E12 Ohm IEC 62631-3-2
Rigidité diélectrique - / 27 kV/mm IEC 60243-1
Indice de résistance au cheminement - / 600 - IEC 60112
Propriétés diversessec / condUnitéNorme du test
Absorption d'eau 9 / * % Sim. to ISO 62
Absorption d'humidité 3.5 / * % Sim. to ISO 62
Masse volumique 1150 / - kg/m³ ISO 1183
Caractéristiques
Transformation
Moulage par injection, Calandrage
Conditionnement
Grains, Couleurs naturelles
Propriétés spéciales
Transparent
Caractéristiques
Propriétés barrière, Copolymère
Résistance Chimique
Stabilité hydrolytique
Certifications
Contact alimentaire, FDA 21 CFR approbation
Applications
Automobile, Électrotechnique et électrique, Médical, Emballage
Disponibilité régionale
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.