Caractéristiques des transformations/physiques | Valeur | Unité | Norme du test |
Other Standards[S] |
Retrait au moulage , parallèle |
0.002 |
mm/mm |
|
Retrait au moulage, perpendiculaire |
0.005 |
mm/mm |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés mécaniques | Valeur | Unité | Norme du test |
Other Standards[S] |
Module de traction |
150 |
MPa |
|
Résistance de compression |
110 |
MPa |
|
Module de flexion |
17000 |
MPa |
|
Résistance à la flexion |
220 |
MPa |
|
Dureté Rockwell |
R 110 |
- |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés thermiques | Valeur | Unité | Norme du test |
ASTM Data |
UL 94 inflammabilité |
V-0 |
- |
UL 94 |
Épaisseur testée |
2 |
mm |
- |
Other Standards[S] |
coefficient de dilatation thermique, long. |
18 |
E-6/K |
|
DTUL à 264 psi |
267 |
°C |
|
Température de fusion |
288 |
°C |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés électriques | Valeur | Unité | Norme du test |
Other Standards[S] |
Rigidité diélectrique, peu de temps |
15 |
kV/mm |
|
Constante diélectrique, 1 MHz |
5 |
- |
|
Résistance de la surface |
>1E15 |
Ohm |
|
Résistance volumique |
>1E15 |
Ohm*cm |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Propriétés diverses | Valeur | Unité | Norme du test |
Other Standards[S] |
Densité |
1800 |
kg/m³ |
|
S: | These properties are reported by the producer according standards that are different to our defaults. |
Caractéristiques
Disponibilité régionale
Asia Pacific
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com