Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delrin® 527UV NC010 - POM - DuPont Engineering Polymers

Material Data Center offers the following functions for Delrin® 527UV NC010:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Delrin datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades.

Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.

Delrin® 527UV is a UV-stabilized medium viscosity acetal homopolymer developed for applications in automotive interiors. It represents a dramatic improvement over Delrin® 507 in mechanical performance after prolonged UV exposure and thermal stability.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 13 cm³/10min ISO 1133
Température 190 °C -
Charge 2.16 kg -
Retrait au moulage, parallèle 2.0 % ISO 294-4, 2577
Retrait au moulage, perpendiculaire 1.9 % ISO 294-4, 2577
ASTM Data
Indice de fluidité, MFI 7 g/10min ASTM D 1238
Température 190 °C -
Charge 1.05 kg -
Retrait au moulage , parallèle 0.0205 mm/mm ASTM D 955
Retrait au moulage, perpendiculaire 0.0205 mm/mm ASTM D 955
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 3100 MPa ISO 527
Contrainte d'écoulement 70 MPa ISO 527
Déformation au seuil d'écoulement 15 % ISO 527
Déformation nominale à la rupture 30 % ISO 527
Résistance au choc Charpy, +23°C 260 kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C 260 kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 9 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 8 kJ/m² ISO 179/1eA
ASTM Data
Module en traction 3230 MPa ASTM D 638
Module de traction 67 MPa ASTM D 638
Module de traction d’élasticité 67 MPa ASTM D 638
Allongement d’élasticité 13 % ASTM D 638
Allongement à la rupture 45 % ASTM D 638
Module de flexion 3050 MPa ASTM D 790
Dureté Rockwell R 120 - ASTM D 785
Izod choc avec entaille, 1/8 in 80 J/m ASTM D 256
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de fusion, 10°C/min 178 °C ISO 11357-1/-3
Température de fléchissement s/chrg, 1.80 MPa 90 °C ISO 75-1/-2
Température de fléchissement s/chrg, 0.45 MPa 163 °C ISO 75-1/-2
Température de ramolliss. Vicat, B 160 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 110 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 120 E-6/K ISO 11359-1/-2
Inflammabilité pr. épaisseur h HB class IEC 60695-11-10
Epaisseur de l'éprouvette 0.8 mm -
Yellow Card disponible oui - -
ASTM Data
UL 94 inflammabilité HB - UL 94
Épaisseur testée 0.84 mm -
coefficient de dilatation thermique, long. 121 E-6/K ASTM D 696
Coefficient de dilatation thermique, trav. 120 E-6/K ASTM D 696
DTUL à 66 psi 168 °C ASTM D 648
DTUL à 264 psi 104 °C ASTM D 648
Température de fusion 178 °C ASTM D 3418
Propriétés électriquesValeurUnitéNorme du test
ISO Data
Permittivité relative, 100Hz 3.8 - IEC 62631-2-1
Permittivité relative, 1MHz 3.8 - IEC 62631-2-1
Facteur de pertes, 100Hz 21 E-4 IEC 62631-2-1
Facteur de pertes, 1MHz 56 E-4 IEC 62631-2-1
Résistivité transversale >1E13 Ohm*m IEC 62631-3-1
Résistivité superficielle 2E13 Ohm IEC 62631-3-2
Indice de résistance au cheminement 600 - IEC 60112
ASTM Data
Constante diélectrique, 1 MHz 3.4 - ASTM D 150
Résistance de la surface 6E14 Ohm ASTM D 257
Résistance volumique 1E14 Ohm*cm ASTM D 257
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 1.2 % Sim. to ISO 62
Absorption d'humidité 0.2 % Sim. to ISO 62
Masse volumique 1420 kg/m³ ISO 1183
Densité 1420 kg/m³ ASTM D 792
Fonctions
Viscosité / Vitesse de cisaillement , Delrin® 527UV NC010, POM, DuPont
Contrainte de cisaillement / Vit. de cisaillement , Delrin® 527UV NC010, POM, DuPont
Module de cisaillement dynamique / Température , Delrin® 527UV NC010, POM, DuPont
Contrainte / Déformation , Delrin® 527UV NC010, POM, DuPont
Module sécant / Déformation , Delrin® 527UV NC010, POM, DuPont
Contrainte / Déformation (isochrone) 23°C, Delrin® 527UV NC010, POM, DuPont
Module de fluage / Temps 23°C, Delrin® 527UV NC010, POM, DuPont
Courbe de fluage 23°C, Delrin® 527UV NC010, POM, DuPont
Volume spécifique (pvT) , Delrin® 527UV NC010, POM, DuPont
Module de traction / Température , Delrin® 527UV NC010, POM, DuPont
Caractéristiques
Transformation
Moulage par injection, Extrusion de films, Extrusion de tubes, Extrusion de profilés, Extrusion de plaques, Extrusion de cable, Extrusion (autres)
Conditionnement
Granulés, Couleurs naturelles
Additifs
Lubrifiant, Agent de démoulage
Propriétés spéciales
Modifié choc, Stabilisé à la lumière, Stabilisé aux intempéries
Caractéristiques
Résistance au fluage, Résistance à la fatigue, Stabilité thermique, Soudable, Homopolymère
Applications
Automobile
Disponibilité régionale
Autres informations
Moulages par injection
Drying is recommended, but not necessary for newly opened packaging stored in a dry location.
Follow the drying guidelines above in the following cases:

·         If moisture is above the Processing Moisture Content recommendation,

·         When a resin container is damaged,

·         When the material is not properly stored in a dry place at room temperature, or

·         When packaging stays open for a significant time.

Résistance Chimique
Acides
Acide acétique (masse en 5%) (23°C)
Acide citrique (masse en 10%) (23°C)
Acide lactique (masse en 10%) (23°C)
Acide chlorhydrique (masse en 36%) (23°C)
Acide nitrique (masse en 40%) (23°C)
Acide sulfurique (masse en 38%) (23°C)
Acide sulfurique (masse en 5%) (23°C)
Acide chromique (masse en 40%) (23°C)
Bases
Hydroxyde de soude (masse en 35%) (23°C)
Hydroxyde de soude (masse en 1%) (23°C)
Hydroxyde d'ammoniaque (masse en 10%) (23°C)
Alcool
Isopropanol (23°C)
Méthanol (23°C)
Ethanol (23°C)
Hydrocarbures
n-Hexane (23°C)
Toluene (23°C)
iso-Octane (23°C)
Cetones
Acetone (23°C)
Ethers
Diethyl ether (23°C)
Huiles minérales
Huile moteur multigrade SAE 10W40 (23°C)
Huile moteur multigrade SAE 10W40 (130°C)
Huile engrenage hypoide SAE 80/90 (130°C)
Huile d'isolation (23°C)
Carburants standards
ISO 1817 Liquide 1 (60°C)
ISO 1817 Liquide 2 (60°C)
ISO 1817 Liquide 3 (60°C)
ISO 1817 Liquide 4 (60°C)
Carburant stand. sans alcool (de pref. ISO 1817 liquide C) (23°C)
Carburant stand. avec alcool (de pref. ISO 1817 Liquid 4) (23°C)
Gasoil (pref. ISO 1817 liquide F) (23°C)
Gasoil (pref. ISO 1817 liquide F) (90°C)
Gasoil (pref. ISO 1817 liquide F) (>90°C)
Selts
Chlorure de sodium (masse en 10%) (23°C)
Hypochlorite de soude (masse en 10%) (23°C)
Carbonate de soude (masse en 20%) (23°C)
Carbonate de soude (masse en 2%) (23°C)
Chlorure de zinc (masse en 50%) (23°C)
Autres
Acétate d'éthyle (23°C)
Peroxyde d'hydrogene (23°C)
Liquide de frein DOT N° 4 (130°C)
Ethylene glycol (108°C)
1% nonylphenoxy-polyethyleneoxy dans l'eau (23°C)
50% Acide oléique + 50% d'huile d'olive (23°C)
L'eau (23°C)
L'eau déionisée (90°C)
Phénol (masse en 5%) (23°C)
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.